    In the second post, there is a pretty good description of arc force/inductance.

    http://www.everlastgenerators.com/fo...Re-The-MTS-160

    Edit. here is the post

    "Inductance,( not induction) is a term used in the electrical field (no pun intended). All our MIG welders have adustable inducatance control. It is of course a technical term with lots of detailed scientific jargon attached. Here is the most brief and simple explanation I can find: http://hyperphysics.phy-astr.gsu.edu...ic/induct.html.

    This example probably relates a closely to what it does in our machines as anything. In short circuit welding, when the arc is "shorted" by the filler wire coming into contact with the weld, the current (amps) drops. The wire then begins to heat up by the rise in current until it heats up sufficiently to pinch off and melt into the puddle. While the time by which it takes the current to "rise" is small and happening many times a second, it can be adjusted through adjusting the inductance of the machine. This is called "current rise time". It allows the wire to break off closer or further from the weld, depending upon the setting. Allowing a quicker current rise time (lower inductance), creates a longer stickout (wire breaking near the puddle) which offers deeper penetration with a narrower bead. This is sometimes called a "stiff arc" or even perceived as running too cold (when in excess). Or allowing a longer current rise time (higher inductance), creates a noticeably shorter stickout, with the wire sometimes pinching off just after it leaves the contact tip. This creates a broader, more fluid looking puddle, as the heat seems to increase over a longer period of time. A smoother, lower bead profile will appear as well. Spatter can increase if set to the extreme. The arc will seem to be wider and the puddle will develop a "buttery" feel and look and may appear to be slow to cool. Inductance control is helpful for out of position welding and achieving a desirable bead profile, depending upon the requirements of the joint."
    Last edited by welderdude; 04-22-2012 at 07:04 PM.
    Everlast lx225
    Hobart Handler 210 with spool gun
    Hobart Stickmate LX
    Thermal Arc 400GMS
    40 amp Northern Tools plasma torch
    130 chicago electric tig welder
    90 amp chicago electric flux mig
    10"-22" Grizzly lathe
    15"-5.5" Grizzly vertical end mill

    In need of nice TIG machine. drooling over PowerTig 250ex

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •