Share
Results 1 to 4 of 4

Thread: 6010 Arc Force settings

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. Default 6010 Arc Force settings

    Hello all,

    can anybody tell me the best arc force settings for the 6010 (Fleetweld 5+, 3/32) with the Everlast PowerArc 200 ?

    Thanks in advance !

  2. #2

    Default

    Quote Originally Posted by betokasu View Post
    Hello all,

    can anybody tell me the best arc force settings for the 6010 (Fleetweld 5+, 3/32) with the Everlast PowerArc 200 ?

    Thanks in advance !
    The PowerArc 200 doesn't have arcforce settings,,,it is adaptive,,,you must mean amp settings,,,,try 50 to 60 amps for that size of rod and remember it's not a drag rod like 7014 it has a longer arc gap (dist from rod to metal) slightly greater than 1/8 inch once the arc is struck,,,,that's why they make scrap iron so you can play and practice on pieces until a fellow gets a feeling for different new rods...hope this helps you
    Some of those lies people tell about me, are true

  3. #3
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    I'm saving up for my first welder. Don't have a lot of experience - will be self-taught! I'm looking at entry-level welders so they won't have user-adjustable arc force settings. Is this feature something I should be seriously considering or will adaptive arc force be "good enough"? The jump is pretty big $-wise. Well, for me it is anyways.

  4. #4

    Default

    http://www.hobartwelders.com/elearning/ amps 40-85 DCEP: DC, Electrode Positive (reverse polarity) has the most weld penetration this mite help
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	electrode_chart.jpg 
Views:	1829 
Size:	20.5 KB 
ID:	6369  
    Last edited by Rodsmachineshop; 04-28-2012 at 03:23 AM.
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

Similar Threads

  1. 250ex Arc Force not working?
    By Monty in forum Stick Welding (SMAW)
    Replies: 2
    Last Post: 08-21-2016, 12:58 AM
  2. Arc Force Question
    By plumber in forum Stick Welding (SMAW)
    Replies: 30
    Last Post: 01-23-2013, 02:05 PM
  3. Arc Force
    By Buzz in forum TIG Welding (GTAW/GTAW-P)
    Replies: 7
    Last Post: 01-19-2012, 05:24 AM
  4. A few questions about the ARC Force knob on my 250EX??
    By CGCINC in forum TIG Welding (GTAW/GTAW-P)
    Replies: 7
    Last Post: 12-06-2011, 02:06 AM
  5. What is arc Force?
    By pmill607 in forum General Welding Questions
    Replies: 2
    Last Post: 08-26-2010, 01:09 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •