  1. Default

    Finead are you
    Alberta or BC ?????
    You have to be Canadian because you have a new model 200dx and i have only sent 2 South of the Border so it is easy to keep track.
    Welds look good hope your enjoying the learning curve
    Cheers
    Duncan
    EVERLAST CANADA
    www.everlastwelders.ca
    www.titanwinches.com

    905 637 1637

  2. Default

    Just need to get myself 100% on all the settings and figure out the frosting area around the weld, seems fairly large on the outside edge.
    Last edited by Finhead; 04-25-2012 at 10:49 PM.

Similar Threads

  1. Water cooled 200DX aluminum issues since new
    By Bad1gdsm in forum TIG Welding (GTAW/GTAW-P)
    Replies: 5
    Last Post: 04-16-2018, 02:48 AM
  2. Tig Beginner : setting up Powertig 200dx-d for aluminum Tig
    By projectvr6 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 11
    Last Post: 03-31-2014, 12:28 AM
  3. Replies: 4
    Last Post: 11-09-2012, 01:15 AM
  4. Will Powertig 200dx weld aluminum cans and razor blades ?
    By bnun12 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 4
    Last Post: 06-11-2012, 12:19 AM
  5. Advise settings on a 200DX for aluminum?
    By Joe from NY in forum TIG Welding (GTAW/GTAW-P)
    Replies: 35
    Last Post: 01-24-2012, 11:27 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •