Today made here such bouquet
(will go to Finland as a gift to the person who helped me with delivery of mine рр256)
tomorrow I will paint with a patina.
Today made here such bouquet
(will go to Finland as a gift to the person who helped me with delivery of mine рр256)
tomorrow I will paint with a patina.
Ruslan
EVERLAST Power Tig 255 EXT
EVERLAST PP256
PC300
EWM Pico 162
MERKLE mobimig 180K
SELCO Genesis 352 pme
beautiful. What material thickness. I see roses made from copper due to the ductility, but this looks like sheet steel, and some aluminum? I would be curious how you formed and more details. Thank you for sharing.
UNT 520D plasma/stick/tig; Hobart Handler 140 Mig; HF 80amp stick welder; Victor O/A; 4x6 Horizontal bandsaw; Planishing hammer; & Stuff
Ruslan
EVERLAST Power Tig 255 EXT
EVERLAST PP256
PC300
EWM Pico 162
MERKLE mobimig 180K
SELCO Genesis 352 pme
Man O man, you have a wonderful ability to take metal and bring it to life!
Very, Very nice!
PowerTig 250EX
Power I-MIG 200
Power Plasma 50
It's what you learn, After you know it all, that counts!
That's what I call the art! The roses are great!
finished article
Ruslan
EVERLAST Power Tig 255 EXT
EVERLAST PP256
PC300
EWM Pico 162
MERKLE mobimig 180K
SELCO Genesis 352 pme
Once again, some gorgeous work, Donor.
Extremely envious of your diverse talents!
Everlast PowerTig 200DX
Everlast PowerPlasma 50
Old 90 amp flux core wire feed
HF 90/160 Amp TIG/Stick
Mini Lathe, Mini Mill, Manual Bender, Ring Roller
HF 2HP 29 Gallon Belt Drive Compressor
8" plate shear, homemade 3-4 ton bench punch
Homemade H-frame press, aluminum casting furnace
HF 12 speed 3/4hp Drill Press, Clarke 4x6 bandsaw
Chop saw, 10" disc sander, 10" Mitre saw modified for aluminum
Makita for the power tools that matter, HF for the ones that dont (or are too expensive)
NICE!! How much time do you have in making that?
http://www.facebook.com/CBRMetalworks
'96 Tacoma V6 on 37's, full custom, built for racin!
Yamaha Rhino w/ 800 Rotax built for racin!
Miller 251 MIG
Everlast Powerplasma 60C with CNC plasma table
Looking for sponsors for KOH 2013 race!
Racin' Tacoma Build Thread
Very nice as all your projects are. Do not think I have seen a bad one yet.
Never in my lifetime would I think I'd be saying "looks the beatiful those roses are!"
Might go youtube the rose making. If not hard, maybe make on for the wife as all shes seews are trucks, bikes, trailers, etc.
Or might be easier to pay Donor to make it (smarter idea hahaha).
Mike R.
Email: admineverlast@everlastwelders.com
www.everlastgenerators.com
www.everlastwelders.com
877-755-9353 x203
M-F 12 - 7PM PST
FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.
Damn! If I could do work like that, the wife might not be so upset at me spending all my money on welding machines!I hope you won the favor of your lady friend.The only thing I might suggest is a spot for a nice candle or two in the middle. Women seem to love candles about as much as they love roses, and a simple pedestal in the center would be easy for someone of your skills. You'd be getting the mad lovin' all day long!
~Joe
Avoid Sears Home Improvement!
Machines
- Lincoln Invertec V100 with TIG
- Ready Welder
- Lincoln Ranger 8 (gone)
I've been doing flowers for a while now have a look at mine in the gallery ;-)
Powertig 200DX
Lincoln 180c
Hobart Handler 125
Miller Thunderbolt
and a bunch of other tools
I just uploaded a pic of a double rose I made for my granddaughter on her 12th birthday ... have a look ;-)
Powertig 200DX
Lincoln 180c
Hobart Handler 125
Miller Thunderbolt
and a bunch of other tools
Is it OK to want to break something just so that you can weld it back together?
Everlast PowerTIG 185 Micro IGBT AC/DC Welder
take a look at the Vietnam vet tribute rose I made (in the gallery) it took about about 3 to 4 hours.
Powertig 200DX
Lincoln 180c
Hobart Handler 125
Miller Thunderbolt
and a bunch of other tools
That really is outstanding ... good job!
Powertig 200DX
Lincoln 180c
Hobart Handler 125
Miller Thunderbolt
and a bunch of other tools
Winky you should do a video on do a rose it would be cool to see how you do it really like the black roses with the gold
EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list
Rod ... I wish I could take credit for the black one with gold ... it was done by JP2CODE I did all the others ... (go to the gallery to see them) they are pretty easy. I take 22 gage sheet metal cut two circles then slit them into the center about 3/4 of the way in ... lay the circles on top of each other drill a hole ... peen a piece of 1/8" round stock insert then weld the top and bottom ... bend the petals up and shape them ... cut out the leaves ... weld it all together ... bend to shape then paint ... clear coat and if I add gold high lights I add that on top of the clear coat so it will reflect the light. I just got a plasma unit so now I'm going to start cutting out the parts with it to give them that rough look ... Maybe I will make a video of that sometime.
Last edited by Winky; 05-08-2012 at 06:40 AM. Reason: spelling
Powertig 200DX
Lincoln 180c
Hobart Handler 125
Miller Thunderbolt
and a bunch of other tools
I think I may have goofed up when I posted the roses I made to this thread ... don't get my feeble attempt at making roses confused with the first one posted ... his bronze colored roses are much better than mine and his deserve to win ... I'm sorry I didn't mean to take any attention away from your beautiful project. I feel like such an idiot sometimes when I use a computer because I am so ignorant when it comes to protocal.
Last edited by Winky; 05-11-2012 at 02:18 PM.
Powertig 200DX
Lincoln 180c
Hobart Handler 125
Miller Thunderbolt
and a bunch of other tools