  1. Default Powertig 185 cannot melt metals

    I was just having problems with my PowerTig 185 machine.
    fire looks weak and cannot melt metals. I've tried to raise high amps but still it looks like a tiny spark.
    anyone here can help me to solve the problem.
    thank you very much for all the responses and suggestion.

  2. #2

    Default

    check your ground first is the metal clean were your ground clamp is
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  3. #3

    Default

    It sounds as if you need to readjust the points. You are only getting HF and the arc is not transferring properly. The readjustment is given in the 185 manual.
    http://www.everlastgenerators.com/do...-185-Micro.pdf

    See Page 26.

  4. Default

    Quote Originally Posted by performance View Post
    It sounds as if you need to readjust the points. You are only getting HF and the arc is not transferring properly. The readjustment is given in the 185 manual.
    http://www.everlastgenerators.com/do...-185-Micro.pdf

    See Page 26.

    I have checked the point gap but the machine still weak spark. When I pressed the trigger I saw a light in the point.
    Should I readjust the point or there something else should I check?

    Thanks
    Last edited by judy; 04-18-2012 at 12:10 PM.

  5. Default

    Quote Originally Posted by performance View Post
    It sounds as if you need to readjust the points. You are only getting HF and the arc is not transferring properly. The readjustment is given in the 185 manual.
    http://www.everlastgenerators.com/do...-185-Micro.pdf

    See Page 26.
    My friend say that may be the capacitors is weak. Is it possible? Or my adjustment incorrect?
    Need advice

  6. #6

    Default

    Quote Originally Posted by judy View Post
    My friend say that may be the capacitors is weak. Is it possible? Or my adjustment incorrect?
    Need advice
    Judy IIRC, the point gap should be glowing blue (ionized air) when the torch is not engaged and the gap should be extinguished when the torch is being used.

    Sounds like you gap is too tight... It needs to be about 0.030" or the thickness of a credit card.
    __________________________
    Everlast Power I-MIG 200
    Everlast PowerUltra 205P
    Everlast SM 200-N
    Thermal Dynamics Cutmaster 42

  7. #7

    Default

    they could be dirty to mine goofed up last year and was just because contact was dirty use some crc contact cleaner on a piece of paper slid the paper between contacts and worked perfect . . a credit card is about the perfect thinness for a gauge a credit card is .025 thick . safer since plastic never use a metal feeler gauge when setting contacts it scratch the points pluss chance of getting shocked using metal . hey talking contacts lol was over at my buddy welding shop he had a old very old tig welder with the cover off it used a spark plug as its contacts sorta cool lol just was a double platinum spark plug
    Last edited by Rodsmachineshop; 04-19-2012 at 01:33 AM.
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  8. Default

    Quote Originally Posted by Rodsmachineshop View Post
    they could be dirty to mine goofed up last year and was just because contact was dirty use some crc contact cleaner on a piece of paper slid the paper between contacts and worked perfect . . a credit card is about the perfect thinness for a gauge a credit card is .025 thick . safer since plastic never use a metal feeler gauge when setting contacts it scratch the points pluss chance of getting shocked using metal . hey talking contacts lol was over at my buddy welding shop he had a old very old tig welder with the cover off it used a spark plug as its contacts sorta cool lol just was a double platinum spark plug
    I've tried again to readjustment the point gap in accordance the instructions.
    I also clean the points with contact cleaner. But my tig still does not work, still weak spark.
    And when I press the trigger I saw the green LED on bottom left side at the IGBT board is off. The three other LED is on.
    is it any relation with the LED indicator?
    So what the problem with my Tig.


    Click image for larger version. 

Name:	PB220623.jpg 
Views:	601 
Size:	107.2 KB 
ID:	6305

  9. #9

    Default

    Quote Originally Posted by judy View Post
    I've tried again to readjustment the point gap in accordance the instructions.
    I also clean the points with contact cleaner. But my tig still does not work, still weak spark.
    And when I press the trigger I saw the green LED on bottom left side at the IGBT board is off. The three other LED is on.
    is it any relation with the LED indicator?
    So what the problem with my Tig.


    Click image for larger version. 

Name:	PB220623.jpg 
Views:	601 
Size:	107.2 KB 
ID:	6305
    You have cold solder joints located on the bottom of your picture - X5 and X6 areas. While they "may" not be your problem, they still should be fixed...
    Last edited by kenwhite; 04-21-2012 at 02:21 PM.
    __________________________
    Everlast Power I-MIG 200
    Everlast PowerUltra 205P
    Everlast SM 200-N
    Thermal Dynamics Cutmaster 42

  10. #10
    Join Date
    Mar 2012
    Location
    Darwin/ Northern Territory/ Australia
    Posts
    40
    Blog Entries
    1

    Default

    Quote Originally Posted by judy View Post
    I was just having problems with my PowerTig 185 machine.
    fire looks weak and cannot melt metals. I've tried to raise high amps but still it looks like a tiny spark.
    anyone here can help me to solve the problem.
    thank you very much for all the responses and suggestion.
    Hi Judy
    Do you have your Gas turned on?
    Had the same problem today with my 250ex(had a welding break and fogot to turn gas back on) Bugger
    Burnt out my gaslens etc.
    Cheers
    Scotty


    250ex
    W 300
    CAT D4D Dozer 49J
    Welded Products Brake Press 30 Tonne
    Tos-Hostivar Tool & Cutter Grinder
    Invicta Major shaper (1.2m stroke)
    Oldfield & Schofield (lathe 1941 young) 5m bed,1.2m gap swing
    CIG Transmig 275
    Lincoln Weldanpower 225DC + 3.5kw 240AC v (Diesel Powered)

  11. Default

    Quote Originally Posted by Rodsmachineshop View Post
    they could be dirty to mine goofed up last year and was just because contact was dirty use some crc contact cleaner on a piece of paper slid the paper between contacts and worked perfect . . a credit card is about the perfect thinness for a gauge a credit card is .025 thick . safer since plastic never use a metal feeler gauge when setting contacts it scratch the points pluss chance of getting shocked using metal . hey talking contacts lol was over at my buddy welding shop he had a old very old tig welder with the cover off it used a spark plug as its contacts sorta cool lol just was a double platinum spark plug
    My dad built some sort of tig welder a while back that used spark plug(s) as well. Was pretty wild

    Although his creation worked like crap and wasn't reality worth the time it took to build it, lol
    New to welding!
    Lots of Snap-On tools
    In need of more toys

Similar Threads

  1. My favorite settings for various cuts, metals and thickness
    By ducksface in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 2
    Last Post: 04-28-2011, 08:27 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •