Quote Originally Posted by sportbike View Post
How much argon flow do you have?

The puddle should be frozen pretty much as soon as you move.
Using approximately 15CFH - acording to the gauge that came with the PP 205, about 7.5 (CFH x 0.472). Too much? Not enough?