Originally Posted by
everlastsupport
What we do.
$40-45/hour MIG (steel) or Stick they bring to us.
$75/hour TIG (steel or aluminum) they bring to us, Mobile MIG (flux core, generator)
$40+ Small jobs, they drop off and pick up, you have to eyeball it.
Crack in lawn mower deck $40 or rusted out dump truck bed or pool cleaners trailer, well eyeball those. Last dump bed was $250 to patch the sides. $42 in steel.
I believe Jody (weldingstipsandtricks.com) did a video or page on pricing. Might google for that too.
Now that sounds pretty good!
I don't want to price it too high but I also don't need practice, I need money!
PowerTig 250EX
Power I-MIG 200
Power Plasma 50
It's what you learn, After you know it all, that counts!