    Quote Originally Posted by CGCINC View Post
    After months of working with Aluminum only, I found it difficult to Tig mild Steel at first.
    I would say, the mild steel is more flexible for TIG welding. Aluminium cannot be welded without a filler rod (I cannot do that for sure), and one is very sensible for temperature, so you have to preheat the parts or you should use a pedal to control current. On other hand, I use to weld some tools made of mild steel without a filler rod using 2T mode and it really works.




  2. #22

    Default

    Quote Originally Posted by FordSloman View Post
    Aluminium cannot be welded without a filler rod
    I Tig welded this Aluminum box in welding class without filler rod. It was 1/8" material with an overlapping corner joint and I just pulse welded it using the extra material overlapping for filler

    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  3. #23

    Default

    Quote Originally Posted by CGCINC View Post
    I Tig welded this Aluminum box in welding class without filler rod.
    It's a nice box! I will try to weld aluminium corner w/o a filler rod someday. Did you try to weld such seams w/o pulse or this is the only way to make the magic? Btw, which pulse mode did you use? I believe it was HI pulse >100Hz?
    The only joint I could weld w/o a filler rod is an edge joint, and a butt joint cracked right after I finished to weld. So, I suppose it could be done technically, but it might be not reliable.

  4. #24

    Default

    that looks awesome really nice welds. the pulse is really nice i sure like it on my 250ex
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  5. #25

    Default

    lol i have not even welded steel with my 250ex and have had it for over 2 years now
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  6. #26

    Default

    Quote Originally Posted by Rodsmachineshop View Post
    lol i have not even welded steel with my 250ex and have had it for over 2 years now
    What do you weld with it? Just Aluminum
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  7. #27

    Default

    yes mostly cylinder heads that are cracked . lots of boat and jet ski exhaust and thick aluminum , most steel i stick or mig lots of cast iron also with stick . if i had the bucks would like a spray welder to do cast iron spray weld like about 20 thousand dollarsClick image for larger version. 

Name:	MillerBP400.jpg 
Views:	354 
Size:	25.9 KB 
ID:	6226
    Last edited by Rodsmachineshop; 04-13-2012 at 07:04 PM.
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

Similar Threads

  1. Finished my Welding cart
    By Ron of Va in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 15
    Last Post: 11-16-2013, 04:07 PM
  2. Recieved my 2013 250EX today!
    By xalky in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 03-08-2013, 01:43 PM
  3. finished plasma tracer
    By Rodsmachineshop in forum Tips & Tricks, Custom Tools, Safety, Ideas and Reviews.
    Replies: 8
    Last Post: 07-02-2012, 12:12 AM
  4. Finished my first Tig Project with pics
    By Buggy Chief in forum TIG Welding (GTAW/GTAW-P)
    Replies: 6
    Last Post: 04-15-2012, 02:35 PM
  5. Hooking up water cooler....Help... Hose to short?
    By CGCINC in forum General Welder Questions
    Replies: 6
    Last Post: 11-09-2011, 05:07 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •