  1. Default PowerTig 225 LX Alu Setup

    Hello Everyone

    I got my everlast PowerTig 225LX for a couple of years now and i never got it to work (((

    Would would be good startig setting to put beeds on a 1/8 thick ALU plate ??
    I have a 1/16 red tungston with a number 6 cup

    What would i set the gas at ?? and just to make sure the ground clamp would be on the ( + ) side and the Tig Toutch would be on the ( - ) ????
    And what would i set all them fancy buttons on the front of the machine ???

    Thanks everyone
    Biggs

  2. #2

    Default

    A 3/32 tungsten would be better.
    I'd start at about 110 amps for just putting beads on a plate.
    Gas at 6 liters per hour on the supplied flowmeter.
    Assuming you are using the pedal, leave the pulse and most of the other knobs off for now, weld in AC.
    Set post flow to be on for about 3-4 seconds to help preserve your tungsten.
    Put the AC Balance at about the 9-10 o'clock position. This will be a little easier to get the puddle to be smoother as it will provide some cleaning.
    AC frequency at about the middle of the adjustment.

    Keep the tungsten close to the puddle, but don't let it touch the puddle or it will contaminate teh tungsten.
    John
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

  3. Default

    I dont think i have any 3/32 do you think 1/8 is alright to start ??

  4. #4

    Default

    Quote Originally Posted by Biggermens View Post
    I dont think i have any 3/32 do you think 1/8 is alright to start ??
    It will probably be fine since your just trying to run beads. I would go to welding tips and tricks and watch his inverter settings video series. I watched them all about three times, and finally sat down with a notebook and took notes. I followed all of his settings. In the video he tells you how he set the machine and then gives a middle of the road number. I used the middle of the road settings first and got to where I could run a bead. After I got better I played around with the settings to see how it changed the weld.
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  5. #5

    Default

    I went to the manual section and down loaded the manual then ran some copys of the front of welder off on printer , so when i am welding different stuff i can see were i had the knobs set . or was set at . i just marked on the picture on the knobs were i had them set for later reference . also always clean your aluminum very well for nice welds i use the heck out of scotch brite pads and stainless steel brushes here a good thing if you ever have nasty dirty aluminum works great for clean and steel also . http://users.eastlink.ca/~pspencer/n...ctrolysis.html washing soda and a battery charger is all you need . save a lot of rusty gas cans and motor cycle tanks doing this
    Last edited by Rodsmachineshop; 04-09-2012 at 07:01 PM.
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  6. #6

    Default

    welding tips and tricks is a great site always watching there videos
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

Similar Threads

  1. 205 pro setup help ??
    By braveops in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 6
    Last Post: 01-06-2013, 04:09 PM
  2. new powertig 185 stick setup
    By jdreich in forum Stick Welding (SMAW)
    Replies: 12
    Last Post: 12-04-2012, 09:25 PM
  3. PP 205 Setup and getting started.
    By qcksnake in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 5
    Last Post: 12-30-2011, 01:40 AM
  4. Tell us about your OXY/ACETYLENE setup!
    By hooda in forum General Welder Questions
    Replies: 6
    Last Post: 05-02-2011, 09:48 PM
  5. New CT520D Setup Help
    By poooorsche in forum Everlast Plasma Cutters (PAC)
    Replies: 3
    Last Post: 06-05-2009, 09:31 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •