Share
Results 1 to 3 of 3

Thread: How Do You Avoid BBs ?

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. #1

    Default How Do You Avoid BBs ?

    Please list your tips to avoid making BBs and get the best possible MIG weld on steel.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  2. #2
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    BBs have a couple of possible causes:
    ~ voltage too high
    ~ wire feed too fast
    ~ too much stickout

    Additionally I found this at the Bernard site:
    http://www.bernardwelds.com/articles/article26.htm

    "Like porosity, insufficient shielding gas and/or dirty base materials can cause spatter. As necessary, increase the shielding gas flow at the regulator and minimize drafts near the welding arc, clean and dry the welding wire, and remove all grease, dirt and other contaminants from the base metal.

    Other factors that can cause spatter are: the wrong size contact tip, a worn contact tip or the wrong tip to nozzle recess. Be certain you have the right contact tips, nozzles and recess parameters for the application."
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  3. #3

    Default

    Use the arc force control to manage this. Additionally, check you gas flow rate. I use a higher content of argon, which reduces the amount of spatter greatly. I use a C18. Much smoother, and cleaner welds.