I've been practicing my aluminum welding and ran into a few things that I don't understand. First is this popping noise I get occasionally from the arc. It doesn't seem to affect the weld. Another issue I have is that sometimes the arc is tight and small and I can get small consistent beads and sometimes the arc seems to spread and has a green hue and make a huge wide puddle and the bead ends up flat and wide. I'm not adjusting anything. I'm going to grab some more scrap from work and run some more beads so I can take pictures Monday. I ended up welding over the welds and sorta erased my evidence. doh!