    Is there a stats sheet and price list out on all of your new lineup yet?

    It's getting close to Xmas bonus time. If my boss thinks I was a very good boy this year, I just may be able to swing a new mig.

  2. #2

    Default

    Quote Originally Posted by roadymi View Post
    Is there a stats sheet and price list out on all of your new lineup yet?

    It's getting close to Xmas bonus time. If my boss thinks I was a very good boy this year, I just may be able to swing a new mig.
    You'll need to call the sales office or check the website for the price. Website is normally delayed. Attached should be the spec sheet.
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	Power-I-MIG-NEW.jpg 
Views:	459 
Size:	88.0 KB 
ID:	160   Click image for larger version. 

Name:	Power-I-MIG2-NEW.jpg 
Views:	515 
Size:	98.1 KB 
ID:	161  
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  3. Default

    Just my 2 cents worth, but I've had a MIG250D since Feb and have yet to find anything it couldn't do. I've never had it over heat, or have a feed problem, or any other issue.

    It's a great machine and will keep on burning wire long after your asleep!

Similar Threads

  1. Everlast migs
    By bobwills in forum General Welder Questions
    Replies: 11
    Last Post: 03-27-2012, 06:05 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •