  1. #1

    Default Noob TIG welds

    In traditional Everlast forums fashion, I submit to the group my first TIG welds from my PPro 256. Don't laugh too hard .

    Click image for larger version. 

Name:	photo(6).jpg 
Views:	402 
Size:	145.0 KB 
ID:	6039

    These were done on 1/16" sheet steel with a 1/16" 2% ceriated, DCEP at 50amps. The steel, only just yesterday, was edging a flower bed, so I cleaned it up as best I could and decided to practice on it. I did notice what I believed to be contamination in the puddle, which almost looked like rust spots, floating up from the leading edge. Anyways, tell me what you think. Constructive criticism is always welcome.

    Thanks
    Mike
    Last edited by posixPilot; 03-26-2012 at 03:33 AM.
    Power Pro 256

Similar Threads

  1. tig noob in need of some help
    By steve1989 in forum General Welding Questions
    Replies: 10
    Last Post: 12-31-2013, 01:15 AM
  2. Noob in need of help
    By Chuck_jkl in forum Introduce Yourself
    Replies: 10
    Last Post: 01-24-2013, 01:17 AM
  3. noob
    By bubbas55 in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 4
    Last Post: 11-08-2012, 12:23 AM
  4. Noob to Tig
    By Ram48 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 7
    Last Post: 04-06-2011, 03:46 AM
  5. Noob from CT
    By Bikenstitchz in forum Introduce Yourself
    Replies: 3
    Last Post: 03-26-2011, 02:13 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •