Would you get the 10' or 15' spool gun? I could save $40 if I go with the shorter one.
I'm not even sure I'll use it but I would like the option of running Aluminum wire.
Would you get the 10' or 15' spool gun? I could save $40 if I go with the shorter one.
I'm not even sure I'll use it but I would like the option of running Aluminum wire.
Last edited by CGCINC; 04-02-2012 at 06:52 PM.
PowerTig 250EX
Power I-MIG 200
Power Plasma 50
It's what you learn, After you know it all, that counts!
Maybe we could also expand the discussion to include, "do you need to match a spool gun to the machine or application" because I notice the Everlast spool guns feature different duty cycles. It may also expand your capabilities with MIG, since these will also weld steel and stainless, and may allow a slightly wider range of wire sizes.
CGC, have you used GMAW on aluminum before? I'd be curious to hear from somebody that has, and what their results have been.
DaveO
Oxweld oxy acet gear
IMIG 200
PowerTIG 210 EXT... Amazing!
PowerTig 250EX
Power I-MIG 200
Power Plasma 50
It's what you learn, After you know it all, that counts!
,,,the whole idea of having a spool gun is to give you the option to weld away from your machine,,, get the longest leads that you can get ,,the 200 amp SM-200m with 20 foot leads is the only way to go,,, it costs more but then how many do you want to buy,,,I don't use mine on aluminium but I do use it on steel
Some of those lies people tell about me, are true
I second that I just added a 15for mig gun to my 205 and I am glad I did, I do not feel tied to the machine anymore It always seemed to be in the way or I was moving the work to get at it.
I also have the 20ft 200 spool gun and like it. By the way Welding direct stocks the consumables for that spool gun, Nozzles, diffusers and insulators along with tips are as mentioned by Geezer elsewhere are from the Binzel 24 KD
Last edited by Ram48; 04-02-2012 at 08:48 PM. Reason: spelling or lack thereof
Everlast I mig 205
Everlast 200 amp spool gun
Everlast 250 ex
H. F. 12x36 lathe
Grizzly Mill
10,000 lb two post lift
Box and Pan Brake
Bead roller
jet 5x7 horizontal band saw
Wilton 14 inch vertical band saw
Mitec 50 A plasma cutter.
tool grinder
20 ton press and press brake
more power and hand tools then I can list here
Dodge Neon that runs 10.23 @143 mph in the quater
70 Chevelle convert
It took 62 years But I finally have my dream Garage
I actually screwed up... I was looking at replace torches for the Mig as well as Spool guns and mixed up the length of hoses. Both spool guns for the IMIG 200 are 20' long.
Because of the size wire you can run through it or is there more reasons?geezer - the 200 amp SM-200m with 20 foot leads is the only way to go