    Default Project 1 from Hooda. Category: 3) Custom Automotive on/off road Welding.

    Howdy Folks, I'm gonna start out with a project that I believe fits into this category. I have a 7,000 lb car hauler From Paiute Trailers' Outlaw series. Good trailer, but very basic. Tandem axle, electric brakes on both axles. And the most annoying ramp stowage system I've ever busted a knuckle on. But that's a different story/project. For now, What I'm doing is mounting a Trailer-Hitch receiver-style mount for my winch, so that I don't have to leave the winch outside with the trailer and a big "STEAL ME" sign on it. Here's pics of the front of the trailer before work started.







    I will be mounting the receiver about 4" forward from the front edge of the trailer bed on the center member. Thanks to some pointers from another member on another thread, I decided to weld a reinforcement plate across the entire center member. I started out with a piece of 1/4" x 3" , got it sawed to length for a trial fit, and decided it just didn't look beefy enough, so next trip to the steel shop, I picked up a piece of 3/8" x 3" instead. More on that later.

    Below are pics of the winch I picked up. I shopped around town for a winch and had my mind set on a 9,000 lb unit at Northern Tool for $399.00, but didn't have the money at that moment, so, I started thinking, the main purpose of this winch will be to pull ROLLING, non-running vehicles up a set of ramps, NOT pulling an f350 out of a snowy ditch, so I figured that I could save some $$ and go with a lesser powered winch, plus the fact that I wanted to be able to detach it, it would be the difference between lunking around 40lb vs. 80lb. I went to FleetFarm, and checked out the Trakker series that they carry there. They also happen to stock the full line of accessories, including a wireless remote control.
    :
    The 4,000 lb seemed to be about what I will need, so the decision was made. Price: $259.00, plus tax. I went home to do a little research on the unit. I plugged in "Trakker winch 4,000" to the google, and Amazon.com came up with the IDENTICAL unit for $132.00 with free shipping! Next day, I had the funds available on a card, so I went back to Amazon and the price had gone down to $116.00 so I put it in my cart and proceeded to check out. By the time I chacked out, $47.00 in shipping charges magically appeared in my total, and there was nothing I could do to get the original price back, so I checked out with a total of $163.00. Still a savings of over a hundred bucks by the time the strate of MN robs another 6.875% off you in tax. A little more monkeying around with my history page, and there I was, same winch, different company through Amazon. Price:$123.00 with free shipping. I was able to get it ordered at that price and cancel the other order in about 5 minute's time.
    :
    2 days later (yes, 2 DAYS, this NEVER happens for me!), The speedy delivery truck dropped off the winch you see below. The identical init to the one at the local store for more that DOUBLE the price. It pays to shop around.





    Sorry for the photo quality, I'm having camera issues. The winch is pictured with the locally sourced mounting plate-$10.00 and Reciever mount-$16.00. When I went accessory shopping, I also got the wireless remote kit, vehicle cable kit, and quick-attach plug set. An extra to set up in case I need to use the trailer with a different truck. I will sum up a list of all the parts used at the end of the project.
    Last edited by hooda; 03-24-2012 at 06:07 PM.
    "It's not magic it's experimental, kind of like washing your hands after pooping used to be." -House

    Everlast PowerTig 250EX-arrived 1-26-2012
    Everlast PowerCool W300-arrived 1-26-2012
    Everlast PowerTig 185 Micro-arrived 1-26-2012
    Everlast PowerPlasma 70-arrived 1-26-2012
    ESAB MigMaster 250-borrowed
    HyperTherm 151 AKA "The Light Sabre"
    Linde UCC-305-964 lb. of old time water cooled TIG love-SOLD-Bad MOJO
    Purox OXY/ACETYLENE

  2. #2

    Default

    Looks like a good fun project! And not only does it have a "steal me" sign on it, it has an "outlaw" sign on it. lol
    Benjamin

    Owner of IMIG 200 and half owner of Power Plasma 50

    https://www.facebook.com/BenjaminRootPhotography

  3. #3
    Join Date
    Feb 2011
    Location
    Fridley, Minnesota
    Posts
    376

    Default Not quite as "smooth" as I was expecting.

    OK, Let me preface this post with the following disclaimer: I AM NOT A PROFESSIONAL WELDER! I will start a new thread/discussion on that in another topic in the near future.
    :
    So, I still had/have the need to join metal, LOTS of metal, so I'm under the gun to get real good, real fast. That being said, I went about the business of attaching the receiver to my trailer yesterday, and it didn't quite go as I was really hoping. Let's face it, I'm out of practice, and lack the knowledge/experience at this point to make show-stopping welds, but I got the job done, and I'm fully confident that it will hold when I put it to work.
    :
    I started out by doing a little improvisational wiring to get some 240 out to the other side of my shop. The main service box is in the opposite end of the building as the shop, so, I had some 2/2/4 Al wire, a 60 amp breaker, and a 50 amp outlet. I attached the outlet to one end, drilled a 1" hole in my windowsill, ran the wire through, attached the breaker and plugged it into the box, and put the ground wire in the ground lug.



    Outside, I have the welder in my rusty, little red wagon, plugged in, and ready to go.



    I would NOT recommend that anybody EVER try this themselves, but it got me out of a pinch.
    :
    Next, I laid out all my tools, Grinder, wire wheels, grinding wheels, clamps, etc.



    Then came the fun part, or in this case, the not-so-fun part. I was using new, 1/8" 7018 from a new, ESAB container. DCEP, 125 amps, arc force at about the 3 o'clock position. I made a bevel along the bottom edge of the bottom plate to match where the tube on the trailer had a radius, thinking that I would fill this area to flush. I played around with amperage, down to 100, there wasn't enough puddle to work with, up past 150, too hot. I settled in at about 122 amps, but even the "best results weren't the best





    These welds LOOK like crap, but the penetration was good, and because of the appearance, I ended up making multiple passes to fill the gap, then just grinding flush for appearance. If this was an appearance-critical situation, I would have either used a different technique, or hired it out, but it ain't.
    "It's not magic it's experimental, kind of like washing your hands after pooping used to be." -House

    Everlast PowerTig 250EX-arrived 1-26-2012
    Everlast PowerCool W300-arrived 1-26-2012
    Everlast PowerTig 185 Micro-arrived 1-26-2012
    Everlast PowerPlasma 70-arrived 1-26-2012
    ESAB MigMaster 250-borrowed
    HyperTherm 151 AKA "The Light Sabre"
    Linde UCC-305-964 lb. of old time water cooled TIG love-SOLD-Bad MOJO
    Purox OXY/ACETYLENE

  4. #4
    Join Date
    Feb 2011
    Location
    Fridley, Minnesota
    Posts
    376

    Default

    After grinding the welds flush, I went about attaching the receiver to the base plate. This being a corner weld with a flat surface to keep things from falling, things went much smoother.







    The 250EX performed flawlessly, there wasn't even so much as a hiccup from the machine through all this. After I finished welding, I used a 40 grit flap wheel to clean things up a bit.

    Once I finished welding the receiver, it was about dark outside, but I didn't want it to rust overnight, so I primed and painted everything in the dark with a flashlight. When I got up this morning, I brought the winch out and slid it into place, so I could snap a few pics of the finished project.







    Now that the welding part is finished, I need to re-run the wires through the tube, modify and re-attach the jack, and run the power cables for the winch, then I'll be able to pull non-running vehicles or whatever onto the trailer with the push of a button. Sweet!
    "It's not magic it's experimental, kind of like washing your hands after pooping used to be." -House

    Everlast PowerTig 250EX-arrived 1-26-2012
    Everlast PowerCool W300-arrived 1-26-2012
    Everlast PowerTig 185 Micro-arrived 1-26-2012
    Everlast PowerPlasma 70-arrived 1-26-2012
    ESAB MigMaster 250-borrowed
    HyperTherm 151 AKA "The Light Sabre"
    Linde UCC-305-964 lb. of old time water cooled TIG love-SOLD-Bad MOJO
    Purox OXY/ACETYLENE

  5. #5

    Default

    I'd be nice if you could upload pics straight from your computer to the forum so that we could have a larger size while still loading pages fast (for those with a slow connection). It's hard for us middle age guys to see those little pics.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  6. #6
    Join Date
    Feb 2011
    Location
    Fridley, Minnesota
    Posts
    376

    Default

    Quote Originally Posted by zoama585 View Post
    I'd be nice if you could upload pics straight from your computer to the forum so that we could have a larger size while still loading pages fast (for those with a slow connection). It's hard for us middle age guys to see those little pics.
    I use photobucket account that I post these from, and I resize them to be SMALLER on purpose. There's choices and I go down to I think it's 320 x 240. Next post I'll try the next size up. Let me know if it's better.
    "It's not magic it's experimental, kind of like washing your hands after pooping used to be." -House

    Everlast PowerTig 250EX-arrived 1-26-2012
    Everlast PowerCool W300-arrived 1-26-2012
    Everlast PowerTig 185 Micro-arrived 1-26-2012
    Everlast PowerPlasma 70-arrived 1-26-2012
    ESAB MigMaster 250-borrowed
    HyperTherm 151 AKA "The Light Sabre"
    Linde UCC-305-964 lb. of old time water cooled TIG love-SOLD-Bad MOJO
    Purox OXY/ACETYLENE

  7. #7

    Default

    On your 7018 horizontal how are you holding the stinger? Are you level with the plate? Angled above the plate? Angled below the plate? Are you pushing, pulling? The reason I am asking is that 7018 can run some good horizontal beads, but rod angle and position is everything, along with temperature.
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  8. #8

    Default

    What would be optimal angle of rod?
    - PT 250EX
    - PCW300
    - POWERCART 250
    - ENCO MILL/DRILL

  9. #9

    Default

    Quote Originally Posted by Cocao View Post
    What would be optimal angle of rod?
    I would hold the rod at a 45-90 degree angle with the end of the rod facing up and the stinger down. To me 7018 runs better dragging when your welding horizontal overhead with the rod going into your weld surface or joint that you are welding. It will just about run itself when you have it set right.
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

Similar Threads

  1. Project 2 from Rambozo. Category: Automotive On Road Trailer Jack
    By Rambozo in forum Other Custom Fabrications
    Replies: 5
    Last Post: 07-01-2015, 07:56 AM
  2. Replies: 10
    Last Post: 02-19-2013, 01:26 PM
  3. Replies: 28
    Last Post: 12-10-2012, 12:21 AM
  4. Project 2 from Undercut. Category: Custom Automotive
    By undercut in forum Other Custom Fabrications
    Replies: 8
    Last Post: 10-03-2012, 10:38 PM
  5. Replies: 9
    Last Post: 09-28-2012, 09:28 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •