    Default Project 2 MigPlazArc Mean Green Contest: Homemade muffler for Briggs

    Well the original muffler broke off a while back and just a pipe was too loud so...Click image for larger version. 

Name:	100_4587.jpg 
Views:	544 
Size:	137.7 KB 
ID:	5964

    I used two pear cans, crimped one of them and pressed them together for the outside part.
    For the pipe I used a 12" long 1/2" water pipe, (which threads right in to the engine) and drilled 5 rows of 7/32" holes in it. I cut a hole just under 1" in each end of the cans, and packed them full of fiberglass.

    Finished size: 12" by 3" and the can is 6.5" total.


    P.S. I would like to use this as my second project for the contest.
    Last edited by MigPlazArc; 03-31-2012 at 03:58 PM.
    Benjamin

    Owner of IMIG 200 and half owner of Power Plasma 50

    https://www.facebook.com/BenjaminRootPhotography

Similar Threads

  1. Giant Muffler
    By dawjr32223 in forum On Road Fabrication
    Replies: 11
    Last Post: 01-24-2013, 01:41 AM
  2. Replies: 0
    Last Post: 11-29-2012, 03:02 AM
  3. I'm MigPlazArc
    By MigPlazArc in forum Introduce Yourself
    Replies: 6
    Last Post: 09-21-2011, 01:13 PM
  4. VW Camper Van Exhaust/Muffler (jakeru's #7)
    By jakeru in forum On Road Fabrication
    Replies: 0
    Last Post: 06-23-2011, 05:42 AM
  5. Water Cooler (homemade)
    By performance in forum TIG Welding (GTAW/GTAW-P)
    Replies: 3
    Last Post: 07-20-2010, 01:07 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •