I use 3/32 2% ceriated between 80 and 120 amps 90% of the time and the other 10% is 1/6 ceriated <80 amps.
I use 3/32 2% ceriated between 80 and 120 amps 90% of the time and the other 10% is 1/6 ceriated <80 amps.