    Default Tungsten size question.

    Excuse the newbie questions... I do seem to have a lot of them...

    Why do you need different size tungsten? I follow that you should size them to the material thickness. If you are welding thick you need a larger diameter so you don't melt it. Why do you need to size down for thinner metals??

    Thanks Guys.
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

  2. #2

    Default

    Brian,

    I'm new to TIG too, but I believe that the smaller tungsten electrodes can give you better arc control for fine work. The larger tungsten, of course, carries more current for welding thicker material.

    Cheers
    Mike
    Power Pro 256

  3. Default

    1/16" and 3/32" pretty much covers everything I do.
    Vice Grips
    WD-40
    Duct Tape

  4. Default

    I use 2% Lanthanated. Is it prudent to grind both ends of the electrode? I am a noobie and I seem to be grinding more than I am welding

  5. #5
    Join Date
    Oct 2010
    Location
    Nova Scotia, Canada
    Posts
    143

    Default

    Grinding both ends lets you flip the tungsten over and use the other point after you dip it.

    Getting up to regrind it every time you dip it helps teach you not to dip it.

    You're choice!

    EDIT: Ugh, sorry, "Your choice!".
    Last edited by Paul Moir; 03-24-2012 at 05:10 AM.

  6. Default

    great point (no pun intended)

  7. #7

    Default

    Quote Originally Posted by Paul Moir View Post
    Grinding both ends lets you flip the tungsten over and use the other point after you dip it.

    Getting up to regrind it every time you dip it helps teach you not to dip it.

    You're choice!
    Another great tip... (bad pun) thanks.... I never though about grinding both ends.
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

  8. #8

    Default

    The amount of current determines the diameter of the electrode. Otherwise it will burn up if to small. I find 3/32" (2.4mm) lanthanated to be good for 130-210 amps, and go up or down from there.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  9. #9

    Default

    I use 3/32 more for 40-180 amp range. I even use it down to 10 amps or so fairly well, when I need to

  10. #10

    Default

    Quote Originally Posted by performance View Post
    I use 3/32 more for 40-180 amp range. I even use it down to 10 amps or so fairly well, when I need to
    That is good to know... Looks like I was writing a reply when you posted. Trying to figure out what I need to pick up to start with and 3/32 looks to be a good standard to start with.

    Thanks for the replies.... Brian
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

  11. #11
    Join Date
    Mar 2012
    Location
    Remote S. Idaho
    Posts
    53

    Default

    3/32 and 1/16 filler is a good combo for up to about 160 amps. The only time I go down to 1/16 tungsten is to use .035 mig wire on small pits or corners.
    To begin with, sharpen a whole quiver full of tungsten so it's no problem to change to a clean one. Dipping the wick messes things up but it's tempting to step on the pedal and try to use it anyway. It don't work, change to a new sharp one.
    Green silicon grinding wheels used for tungsten carbide tool sharpening works on electrodes.

  12. #12

    Default

    Quote Originally Posted by everlastsupport View Post
    The amount of current determines the diameter of the electrode. Otherwise it will burn up if to small. I find 3/32" (2.4mm) lanthanated to be good for 130-210 amps, and go up or down from there.
    I can follow you can melt a rod if too much current, but how bad is the arc if you are using a large rod for thinner work. You still have a point. Is it really bad to handle or would it just be a little better to use a smaller diameter? Me the logical thinker would say as long as you have the current turned down it should be pretty close. Then you are controlling a temper mental arc. Haha
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

  13. #13

    Default

    Quote Originally Posted by Brian Ski View Post
    I can follow you can melt a rod if too much current, but how bad is the arc if you are using a large rod for thinner work. You still have a point. Is it really bad to handle or would it just be a little better to use a smaller diameter? Me the logical thinker would say as long as you have the current turned down it should be pretty close. Then you are controlling a temper mental arc. Haha
    It could affect the weld width and penetration. I normally keep 3/32" in and it covers what I do. But might not for others. Arc start/control is always fine for me with our units.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  14. #14

    Default

    I find the bigger tungsten will put too much heat out even if the amps are dialed back. It's just a wider path of heat so when you jump down in size on the electrode, it concentrates the heat in a smaller area giving more control of the arc path.
    Once you start Tig'ing you'll instantly understand. I used to think why this, why that but as soon as I got into school and started Tig'ing, within a week, all my questions were answered. (Basically )

    I used 1/8" and 1/16" for the most part. 2% Thoriated. I have some 1.5% Lanthanated but the Thoriated works better for me even though it makes me toxic.
    Last edited by CGCINC; 03-22-2012 at 03:01 PM.
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

Similar Threads

  1. Wire size question...?
    By CGCINC in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 20
    Last Post: 06-15-2012, 01:41 AM
  2. Perhaps a silly question about tungsten...
    By Trip59 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 05-28-2012, 11:25 PM
  3. Tungsten Question
    By SeanMurphy265 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 7
    Last Post: 09-12-2011, 04:22 AM
  4. Tungsten grinder question
    By Ram48 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 6
    Last Post: 09-06-2011, 06:53 PM
  5. collet size vs tungsten size
    By docweathers in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 01-08-2011, 04:31 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •