Share
Results 1 to 3 of 3

Thread: What is 95/5 Argon/Oxygen gas used for???

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. #1

    Default What is 95/5 Argon/Oxygen gas used for???

    I ran across someone selling a cylinder of 95/5 gas. I thought you need to keep oxygen away from your welds???
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

  2. #2

    Default

    I can answer that!!
    I just asked a similar question. Mig welders use mixed gas when welding.
    Oxygen is normally added to argon in amounts of 1%, 2%, or 5%. When oxygen is added to argon, it improves the penetration pattern. It also improves the bead contour and eliminates the undercut at the edge of the weld. You use argon-oxygen mixtures in welding alloy steels, carbon steels, and stainless steel


    There are many different combinations and they are all used for welding different materials.

    http://www.everlastgenerators.com/fo...al-world-input


    .
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  3. #3

    Default

    Oxygen additions can also be added in to make the gas active and actualy strengthen the weld due to intentional oxide formation.
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

Similar Threads

  1. 100 PSI argon flo?????
    By stretch in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 32
    Last Post: 06-09-2016, 08:51 PM
  2. Why 100% Argon or Argon/CO2 75/25%
    By mdennis in forum General Welding Questions
    Replies: 6
    Last Post: 08-09-2013, 04:11 AM
  3. Air/Argon
    By ChadP in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 11
    Last Post: 02-09-2013, 09:20 PM
  4. propane acetylene oxygen
    By Rodsmachineshop in forum General Welding Questions
    Replies: 16
    Last Post: 05-23-2012, 03:46 PM
  5. ARGON and ARGON/CO2 TANK SIZES
    By everlastsupport in forum Technical Bulletins and Tips
    Replies: 47
    Last Post: 10-13-2011, 05:19 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •