75%/25% for mild steel,
I have used tri mix with mild steel, but that was given to me on accident. I believe it's more expensive per bottle.
100% argon for aluminum
75%/25% for mild steel,
I have used tri mix with mild steel, but that was given to me on accident. I believe it's more expensive per bottle.
100% argon for aluminum
Lincoln Eagle Engine Drive
Everlast MTS 250
Everlast Power Tig 225lx
HTP Mig 2400
Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
Miller Spectrum 375 Extreme Plasma cutter
Victor cutting torch
HF 20 Ton Shop Press
HF 4x6 Band Saw
HF Air Compressor
Northern Tool Drill Press
www.murphywelding.com
Thanks for the link to this post... Answers some more questions.
For the MIG I have have been using 75/25 Argon Co2 mix for steel. (That was what the LWS recommended) Been using it ever since. Pretty much all what I use it for (steel).
I did have to do some stainless welding and it worked as well as I could tell. Someone told me I could braze the stainless. Well that was a train wreck!!!! haha
Shade tree MIG welder.
Now a Shade tree TIG welder.
For MIG I use 75/25 Ar/Co2, my son likes Stargon (Prax air tri gas). The Stargon does seem to weld a bit better.
TIG is straight argon for me.
Mike R.