Share
Results 1 to 20 of 45

Thread: New Thread, same topic, my CAREER is on the line, please help ON TOPIC.

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. #1

    Default Hang Tuff

    Hooda you need to take some of the coments from these guys with a grain of salt I am sure that when they started there welds looked as bad as mine and yours there is quite a learning curve to tig welding thats for sure getting right settings and gas flow what size tungsten and filler rod its endless but I do think this can be learned most members here are willing to share there knowledge and advice so hang tuff you may find someone that knows the in's and outs of tig in your area and pay them for a couple hours of there time or a case or two of beer to do a little coaching might be the ticket hang tuff brother things will get better if you are determine to and keep trying good luck
    Bill

  2. #2

    Default

    Jake98, that was funny, too bad you deleted it. Would have maybe brought a little humor to this thread.

    Hooda, if you can leave all the details as the pictures are not clear enough for anyone to go from, many here will give you parameters to get you in the ballpark.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

Similar Threads

  1. Gas line fitting thread?
    By Skeeter in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 04-09-2015, 12:55 AM
  2. New Sub Forum under the Off Topic area
    By brad3579 in forum Truck, Car and Bike builds
    Replies: 3
    Last Post: 02-20-2012, 01:49 PM
  3. Editing thread title, my thread
    By worntorn in forum Forum related Questions
    Replies: 10
    Last Post: 06-20-2011, 08:03 PM
  4. Using a gas Y for Tig purge line
    By worntorn in forum TIG Welding (GTAW/GTAW-P)
    Replies: 12
    Last Post: 03-19-2011, 01:02 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •