Originally Posted by
sydneysdad
Sprocket,
I have the PU205 and all I can say is it's more than I can ask for, yes you don't get all the bells and whistle's but that's not what I need anyway.
By no means am I a welder but I know my capabilities.
back to the pu205. I set my air at 65psi, amps at 45 and I've cut 3/8 steel with no problems at all and the switch to tig is no more the 1 min.
oh and it's on 220v. this machine (to me) is more than you get for the money you pay.
hope that helps.
Have you ever tried your 205P on a 120V branch? I wonder how well yours works on 120V, or if its just the two that I have tried...
__________________________
Everlast Power I-MIG 200
Everlast PowerUltra 205P
Everlast SM 200-N
Thermal Dynamics Cutmaster 42