Okay folks,
Turn on the NOOB lamp.
BRAND NEW PP205 - received it last Friday. Just got it hooked up this evening.
QUESTIONS:
Are there any specific settings on the PowerPro 205 that will cause the unit not to plasma cut? It won't even give me a pilot arc.
When set to CUT, the amp readings are all over the place no matter where you set the dial.
I never get a "CUT" light on the control panel.
My beautiful (worthless) manual says my unit has a switch for "air testing/cut". it does not.
When set to MMA, the stick welder works fine.
Can someone PLEASE tell me where all the knobs should be set on this thing! Is there some mystery switch?
HELP!
CHECKLIST:
* Good Power 241VAC (120 from each HOT lug to ground)
* Good grounds on work
* Good air pressure
* Pre and post flow set to MAX
* HF set to min-max (didn't matter where I set it)
* AMPS set to max, mid-range, etc - readings were not stable at all
WHAT AM I MISSING HERE??!!
Any help appreciated - thanks in advance,
inthefrey