    Ok.. First my lame joke...
    6011 goes both ways
    So 6011 is like a high school cheerleader after her first drink of Peach snopps?! Ba dump, bump!

    Ok, now my real question:
    SPORTBIKE - 7018 is a hassle to deal with and is of very limited benefit to 90% of the welds that are made and is still equal or over-matched to most of the base metals that will be used.
    What do you mean by a hassle?
    And what do you mean by limited benefit?

    I'm learning stuff is why I'm asking.... I've welded with 6010,6011,6013 and 7018 and the 7018 was the easiest to use for me as far just arc characteristics and ease of laying a bead.
    I spent a few days in class with 3/8" plate ground to an angle and doing root passes with the 6010, then fill with 7018. What a pain.
    Last edited by CGCINC; 03-16-2012 at 01:55 AM.
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

Similar Threads

  1. First Welding Project - You guessed it... a welding cart
    By EmptyNester in forum Hobyist Projects
    Replies: 19
    Last Post: 10-12-2011, 04:30 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •