Thread: High pitched beep coming from machine

  1. Default High pitched beep coming from machine

    Hey guys I was playing with my new powerpro 205 multiprocess and as im welding using the TIG process and for some reason today im getting a high pitched beeping noise when im welding. Seems to be more predominate in the pulse setting. No idea what it is but its annoying. Doesnt seem to be affecting the welding but just wanted to make sure it wasnt about to blow up on me or something

  2. Default

    I really dont know anything bout tig but from what I hear it sounds like something going on with the high frequency. Do you use a separate high fequency ground ran to your machine on the back.
    Gabe
    everlast power arc 200
    Lincoln electric 225 tombstone
    lawn mowers

  3. Default

    no i just use the regular ground on front. After using it for a few days it went away, just pops up now and then and like i said, doesnt make a performance difference so i guess ill just roll with it.

  4. Default

    Well maybe try putting your welder near a ground rod and hooking the high frequency ground in the back to the ground rod. Its not necessarily but it is there to reduce the interference.
    Gabe
    everlast power arc 200
    Lincoln electric 225 tombstone
    lawn mowers

  5. #5

    Default

    That is most likely the IGBTs making that noise. I worked on a CAT scanner that had a HV system with IGBTs and at some current setting the would make funny noises. I seem to hear it a low current setting only.

    have fun
    Tom

    Everlast PM256
    Millermatic 180
    Hypertherm PowerMax 65 with machine torch
    Longevity Force Cut 80I
    DIY CNC table for plasma/routing
    13" metal lathe
    Small Mill
    ect, ect.

  6. #6

    Default

    Could also be a coil (choke/inductor) squealing. They look like this... Click image for larger version. 

Name:	coils..chokes.jpg 
Views:	502 
Size:	25.7 KB 
ID:	5818

    Can be diagnosed with a 3 foot length of rubber or vinyl tubing by putting one end to your ear and moving the other end around the suspected area of the sound. When the tube is over the offending part, the sound will be much louder. Don't put your hands close to any shock hazard.

    The remedy is to put a few drops of paraffin wax or clear fingernail polish on the coil to dampen the vibrations and stop the squeal.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  7. Default Thanks

    Thanks guys and thanks zoama585 ill try that this weekend and see how it works!

Similar Threads

  1. Floating head Machine Torch holder w/ S45 Machine Torch - 2 for sale.
    By countryguy in forum Everlast Plasma Cutters (PAC)
    Replies: 2
    Last Post: 12-19-2016, 09:52 PM
  2. 200DX High Amperage Reading (664A) and Machine Will Not Respond
    By Synthetic in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 02-20-2013, 02:54 AM
  3. Getting a high pitched buzz and little or no arc
    By jtybt in forum TIG Welding (GTAW/GTAW-P)
    Replies: 3
    Last Post: 03-02-2011, 09:38 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •