  1. Default

    Ok now Ive got it grounded but for some reason my amps arent staying where I want them. I have it at full 50 amps but when i start cutting (had my wife watch the digital read as i was cutting) it drops to 22 and hangs there causing the cut to take longer. What could be the cause of this?

  2. #2

    Default

    Quote Originally Posted by Jef_Replogle View Post
    Ok now Ive got it grounded but for some reason my amps arent staying where I want them. I have it at full 50 amps but when i start cutting (had my wife watch the digital read as i was cutting) it drops to 22 and hangs there causing the cut to take longer. What could be the cause of this?
    Possibly poor ground.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  3. Default

    Quote Originally Posted by zoama585 View Post
    Possibly poor ground.
    Its latched on there tho... ugh frustrating.. it jumps to 22amps then as soon as i let go of the trigger it creeps back up to 52. Ill play with it some more but that ground is on there and metal is clean.. shouldnt matter that its on hot rolled right? I didnt think the carbon coating would really take away from the ground.

  4. #4

    Default

    Yes, it will drop to 22 amps as long as the pilot arc is in play. When the arc transfers to the metal during the actual cut, it will jump back up. IF not, you may have done damage to the torch or the pilot arc circuit trying to use it without the clamp for so long. The Pilot arc is NOT designed for running continuously as you had done previously.

  5. Default

    Quote Originally Posted by performance View Post
    Yes, it will drop to 22 amps as long as the pilot arc is in play. When the arc transfers to the metal during the actual cut, it will jump back up. IF not, you may have done damage to the torch or the pilot arc circuit trying to use it without the clamp for so long. The Pilot arc is NOT designed for running continuously as you had done previously.
    I did it without a clamp for mere minutes. I didnt continualy use it for days or something without. Ive already emailed customer support I really dont think this is from user error. Im going to be really disapointed if my warranty is voided because i didnt have it grounded for a few short occasions (a mistake every noob makes along with forgetting the gas is not turned on)

  6. Default

    POSTED ON WELD WEB AFTER I GOT OFF WORK AND HAD A CHANCE

    "Thanks for all the input guys and moving it to the right thread. Since i started this thread ive found out a lot and mike the sales rep has brought to my attention that it could be my fault but I hope its not because like assassin_works said im broke as a joke because im married haha.

    The problem started way before I posted on here like a couple days ago. I've been welding for years but not to big on plasma cutting. Just lots of oxy settling burnin'. Well this whole "pilot arc" ordeal was a bewilderment to me because normally on the plasmas ive used in the past if its not grounded its not gonna do more than give u a little arc and go out. Well the pilot arc kept goin and on accident i realized i didnt need the ground to cut through thin sheet metal when i was playing around with it trying it out. Then i realized i do need the ground becuase when it came to thicker material it just wouldnt cut. (biggest noob mistake ever i know) well now they are thinkin Ive ruined the torch and now made it so the pilot just stays on at all times. Reason i didnt come out and say anything about it on here was because i didnt think it was related if you look at my original post I thought i just wasnt running enough power to the unit.

    Not sure if i caused it but just had to clear the air because people on the other forum were accusing me of spamming since i have two different usernames on this and everlast and had two similar threads going. "

  7. #7

    Default

    Jef,
    Don't worry, if there is a problem we will help you out.

  8. #8

    Default

    Quote Originally Posted by Jef_Replogle View Post
    Its latched on there tho... ugh frustrating.. it jumps to 22amps then as soon as i let go of the trigger it creeps back up to 52. Ill play with it some more but that ground is on there and metal is clean.. shouldnt matter that its on hot rolled right? I didnt think the carbon coating would really take away from the ground.
    The mill scale is likely insulating the clamp quite a bit Should be ground off.
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

  9. #9

    Default

    Mere minutes, is enough to melt down a consumable and possibly a torch head. The arc is being carried through the torch body on tiny wires and the being fed back through a sensitive series of circuits. The pilot arc is designed for mere SECONDS of continual use. OE is a large cause of issues. Having a work clamp left over is a should be an immediate warning that something isn't right. 80-100 psi is way too high, and that is discussed in the manual I believe as well as some of the basics. The coating on the steel is mill scale, and probably oil. It can interfere, but not usually if it is fairly clean metal. What model do you have?

  10. Default

    Its a powerpro 205 and yes metal is clean.

  11. #11

    Default

    Is your torch in the negative or positive?

Similar Threads

  1. 256 plasma problems
    By Charkilah in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 2
    Last Post: 11-08-2012, 09:03 PM
  2. Power Plasma 50 plasma cutter....
    By CGCINC in forum Customer Testimonials
    Replies: 4
    Last Post: 07-20-2012, 12:58 PM
  3. Plasma Problems
    By Slartybartfa in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 34
    Last Post: 07-03-2012, 02:03 AM
  4. Problems with plasma cutter
    By Kodiak in forum Everlast Plasma Cutters (PAC)
    Replies: 10
    Last Post: 04-11-2012, 07:19 PM
  5. Problems getting expendables for SG-55 plasma cutter/cable.
    By The_Postman in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 6
    Last Post: 03-21-2012, 05:32 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •