Thanks mark. I got names flipped and accidentally called mike today but after walking him through the problems we came to the conclusion that it wasn't going off the pilot arc (because it was going through the 3/8" steel but the reason it may be losing momentum and getting slaggy was that my compressor is right at the minimum for the machine and may not be keeping up. He said the digital read out isn't always showing right during the cut. Also gonna try a part he recommended for a secondary way to keep water out of the line. Very helpful! Sorry again for all the craziness on here.