  1. #1

    Default

    A little trick a bender showed me when bending thin tubing he would fill tube with fine sand and cap both ends then bend then tubing wouldn't shrink while bending

  2. #2

    Default

    That is some nice work! After you weld everything together will it bolt up easy or does welding tweak it?
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  3. Default

    Quote Originally Posted by Rodsmachineshop View Post
    how thick was the tubing
    The tubing is .065 wall.

    Quote Originally Posted by zoama585 View Post
    Do you ever find the mandrel bend to be smaller than the unbent part of the tube ?
    It is not mandrel bend tubing...this is what I use:



    It is a sanitary fitting, and has the same diameter all the way through. These are perfect.

    Quote Originally Posted by SeanMurphy265 View Post
    That is some nice work! After you weld everything together will it bolt up easy or does welding tweak it?
    The flanges and flex pipe gets welded last, this it to allow for proper fitment. The stainless dos shrink a fair bit when welded.

  4. #4

    Default

    Quote Originally Posted by Boosted P View Post
    The tubing is .065 wall.



    It is not mandrel bend tubing...this is what I use:

    It is a sanitary fitting, and has the same diameter all the way through. These are perfect.
    where would you get this?
    Journeyman welder
    250EX
    Power plasma 60
    horizontal band saw
    Miller digital elite 'wicked' lid

  5. Default

    Quote Originally Posted by jerky View Post
    where would you get this?
    From me

  6. #6

    Default

    Quote Originally Posted by jerky View Post
    where would you get this?
    Google- sanitary fittings butt weld.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  7. Default

    Quote Originally Posted by zoama585 View Post
    Google- sanitary fittings butt weld.
    Nice going, you gave away the greatest secret of all time.....GOOGLE.

  8. #8

    Default

    most stuff i work with is .125 wall tubing with my mandrel bender it doesn't like thin stuff tends to stretch and not stay the same size when bending .065 is thin stuff to bend

  9. #9

    Default

    yes i can use google, but i figured since you in alberta, you have a source close to home.
    Journeyman welder
    250EX
    Power plasma 60
    horizontal band saw
    Miller digital elite 'wicked' lid

  10. Default

    Quote Originally Posted by jerky View Post
    yes i can use google, but i figured since you in alberta, you have a source close to home.
    Well, if you want to buy this stuff in Alberta you will pay 2.5x what you would pay for it down south.

  11. #11

    Default

    Awesome work! I'd like to do headers for my 240Z at some point, there are some on it now but they are not well thought out.

    What are you doing to get such uniform ovals out of the round tubing going into the flanges? Your not just bending them in a vise are you? I would think that would "pinch" the mid-point on the tubing. Are you buying some pre made stuff for that?
    H: PowerTig 250EX
    W: Lincoln Precision Tig 225
    W: MK Products CobraTig 150 orbital welder

Similar Threads

  1. Project #11 From Jason: MK3 AWD 3.4L Twin Turbo Jetta
    By Jason in forum Other Custom Fabrications
    Replies: 21
    Last Post: 06-05-2013, 04:35 AM
  2. Twin turbo mustang intake
    By Zmechanic in forum On Road Fabrication
    Replies: 25
    Last Post: 04-28-2013, 05:46 PM
  3. Project 1 From TT WS6 - Twin Turbo Trans Am
    By tt ws6 in forum On Road Fabrication
    Replies: 6
    Last Post: 12-09-2012, 11:27 AM
  4. Project 1 from Injected65. Twin Turbo Kit
    By Injected65 in forum On Road Fabrication
    Replies: 13
    Last Post: 06-01-2012, 06:39 PM
  5. Replies: 12
    Last Post: 03-10-2011, 07:25 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •