Excellent work. You didn't cut any corners, and it shows. Thanks for sharing!
 
 
		Excellent work. You didn't cut any corners, and it shows. Thanks for sharing!
'13 Everlast 255EXT
'07 Everlast Super200P
 
 
		Wow that is really nice. I wish I could weld half that good. Stainless looks so great.
Do you bend the pipe yourself or get prebent sections and cut to fit... Even the cuts look tight. Thanks for the pictures.
Shade tree MIG welder.
Now a Shade tree TIG welder.
 New Member
					
					
						New Member
					
					
                                        
					
						
							
								 
							
						
					
					
						 
 
		Links to my welding projects > : Spray Arc with the 250p : Coldsaw Stand : Welding Cart : Heavy Duty Rolling Shelf : Taller Bandsaw
2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw
 
 
		if there mandrel bent that should not happen. when tube is crush bent, then the bend does reduce in diamater. thats usually why mandrel bent stuff is more expensive
Journeyman welder
250EX
Power plasma 60
horizontal band saw
Miller digital elite 'wicked' lid
 
 
		Links to my welding projects > : Spray Arc with the 250p : Coldsaw Stand : Welding Cart : Heavy Duty Rolling Shelf : Taller Bandsaw
2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw
 
 
		how thick was the tubing
 
 
		A little trick a bender showed me when bending thin tubing he would fill tube with fine sand and cap both ends then bend then tubing wouldn't shrink while bending
 
 
		That is some nice work! After you weld everything together will it bolt up easy or does welding tweak it?
Lincoln Eagle Engine Drive
Everlast MTS 250
Everlast Power Tig 225lx
HTP Mig 2400
Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
Miller Spectrum 375 Extreme Plasma cutter
Victor cutting torch
HF 20 Ton Shop Press
HF 4x6 Band Saw
HF Air Compressor
Northern Tool Drill Press
www.murphywelding.com
 New Member
					
					
						New Member
					
					
                                        
					
						
							
								 
							
						
					
					
						 
 
		The tubing is .065 wall.
It is not mandrel bend tubing...this is what I use:
It is a sanitary fitting, and has the same diameter all the way through. These are perfect.
The flanges and flex pipe gets welded last, this it to allow for proper fitment. The stainless dos shrink a fair bit when welded.
 New Member
					
					
						New Member
					
					
                                        
					
						
							
								 
							
						
					
					
						 
 
		Links to my welding projects > : Spray Arc with the 250p : Coldsaw Stand : Welding Cart : Heavy Duty Rolling Shelf : Taller Bandsaw
2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw
 New Member
					
					
						New Member
					
					
                                        
					
						
							
								 
							
						
					
					
						 
 
		most stuff i work with is .125 wall tubing with my mandrel bender it doesn't like thin stuff tends to stretch and not stay the same size when bending .065 is thin stuff to bend
 
 
		yes i can use google, but i figured since you in alberta, you have a source close to home.
Journeyman welder
250EX
Power plasma 60
horizontal band saw
Miller digital elite 'wicked' lid
 New Member
					
					
						New Member
					
					
                                        
					
						
							
								 
							
						
					
					
						 
 
		Awesome work! I'd like to do headers for my 240Z at some point, there are some on it now but they are not well thought out.
What are you doing to get such uniform ovals out of the round tubing going into the flanges? Your not just bending them in a vise are you? I would think that would "pinch" the mid-point on the tubing. Are you buying some pre made stuff for that?
H: PowerTig 250EX
W: Lincoln Precision Tig 225
W: MK Products CobraTig 150 orbital welder
 
 
		Do you experience any heat issues with the transmission or other parts? Do you find any value to ceramic coating the hot side tubing or using a turbo heat cover in an application like this? S/F.....Ken M
Lincoln Power MIG 300
Everlast 160STH
Miller 225 Thunderbolt (sold it)
Lincoln Squarewave 175 TIG(traded it for)
Miller DEL 200 welder/genset
Thermal Dynamics 1250XL plasma cutter
Miller XMT300
 
 
		Is it OK to want to break something just so that you can weld it back together?
Everlast PowerTIG 185 Micro IGBT AC/DC Welder