    Well, everybody posts pics of their welding table, so here's mine. This was my first actual welding project since I got my 250EX. I spent a lot of time building my cooler, but there was no welding involved so it didn't count. I should say first that I figured that this would be a good way to get to know the welder and to try to re-learn TIG. I actually received formal TIG training, but its been a long time - I think Nixon was president at the time and they were calling it Heliarc. I was initially repairing chromoly truss work on light aircraft airframes and fixing cracks in inconel exhaust stacks.

    Anyway, I didn't need a big table right now since I'm just piddling around with small projects. I scored a piece of 3/8" plate about 34" x 27" for $30 so that became the right size.

    I had a bunch of 1-1/4 thin wall (1/16") tubing from an old fence we took down, so I used that for the frame. Its a little light for a welding table but I figured since mine is small it would work OK. I decided to bolt the top to it, so I got some DOM and cut some bushings and tacked them in place on the ends of the top rails. This way, I can crank down on the bolts without crushing the tubing.
    Click image for larger version. 

Name:	P2130003.jpg 
Views:	674 
Size:	120.3 KB 
ID:	5704Click image for larger version. 

Name:	P2130004.jpg 
Views:	715 
Size:	140.7 KB 
ID:	5705

    Still got a ways to go with my beads, but I was able to stick it together.
    Click image for larger version. 

Name:	P2130009.jpg 
Views:	679 
Size:	84.3 KB 
ID:	5708Click image for larger version. 

Name:	P2130007.jpg 
Views:	660 
Size:	89.9 KB 
ID:	5707Click image for larger version. 

Name:	P2130006.jpg 
Views:	770 
Size:	95.4 KB 
ID:	5706

    Here's the finished table
    Click image for larger version. 

Name:	P2250001.jpg 
Views:	745 
Size:	106.5 KB 
ID:	5709

    I was debating where to put a holder for the torch, so while I'm deciding, I got some stainless rod and bent it up and tacked it to a piece of angle iron. I stuck some flea market magnets to the angle iron and then stuck that to one leg of the table for now.
    Click image for larger version. 

Name:	P3020003.jpg 
Views:	1788 
Size:	111.3 KB 
ID:	5711Click image for larger version. 

Name:	P3020005.jpg 
Views:	1328 
Size:	113.0 KB 
ID:	5712Click image for larger version. 

Name:	P3020006.jpg 
Views:	1910 
Size:	107.1 KB 
ID:	5703

    Here's my welder and homemade cooler set up. My next project needs to be a welding cart so I can give my wife her garden cart back.
    Click image for larger version. 

Name:	P2250002.jpg 
Views:	1101 
Size:	138.4 KB 
ID:	5710

    Regards,
    -RP

  2. #2

    Default

    I like it how you left room to fit your feet under the table. I did the same with mine. The hook it cool too. I hang mine over the ground clamp but I'm thinking about making a hook after seeing yours.
    Everlast PowerTig 250EX
    Everlast PowerCool 300
    Everlast PowerPlasma 70
    Lincoln Powermig 215
    Magnum SG Spool Gun
    Don't jump on my Gomba

  3. #3

    Default

    That garden cart actually fits everything pretty good...

    Your table looks really nice and adding bushings for the bolts was a great foresight!
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

Similar Threads

  1. Tig Welding Table
    By knock10090 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 9
    Last Post: 02-22-2015, 03:17 AM
  2. Welding table
    By joshuab in forum Other Custom Fabrications
    Replies: 12
    Last Post: 02-26-2014, 12:30 PM
  3. New 4' x 6' Welding Table
    By Rafael in forum Other Custom Fabrications
    Replies: 16
    Last Post: 07-16-2013, 02:23 PM
  4. Project # 2 Welding table
    By yotarover in forum Personal Projects (no welder required)
    Replies: 0
    Last Post: 06-03-2011, 03:47 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •