I've been out in the shop this morning measuring wire speed on my I-MIG 250p at every setting. I'm making myself a chart since there's nothing on the machine to indicate wire speed.
I've found that max wire speed is way below the 700ipm spec at 432ipm. I have an 11Lb roll of .035 steel wire on the machine, there's no tension on the roll since you can only tension a 33LB/44LB roll due to design.
The drive roller tension is set to 3 front and rear. This is the minimum tension for consistent feed (no slippage of the feed rollers) tested by pulling the trigger with the gun against the table at a 45 degree angle.
With the "amp" dial pointing straight up to 140, I get 210ipm. Pointing to 250 I get 380ipm. Turned fully to the right (max) I get 432ipm.
The machine is running on 240v measured at the plug.