    Default

    I worked my way up the piece. Sometimes having to make spacer blocks to keep the bars parallel. Overall, it worked out. Not as seamlessly as I had dreamed of last night, but hey I can't complain. So here's the final shot of the structure all tacked up and ready for some finish welding. I think I'll save that for another day. I've got a few other projects burning that need some attention too!

    Click image for larger version. 

Name:	2012-03-03_11-39-03_234.jpg 
Views:	352 
Size:	132.1 KB 
ID:	5664Click image for larger version. 

Name:	2012-03-03_11-58-18_55.jpg 
Views:	380 
Size:	140.7 KB 
ID:	5665Click image for larger version. 

Name:	2012-03-03_12-05-07_265.jpg 
Views:	378 
Size:	141.5 KB 
ID:	5666
    d.fisher, dedicated to art and craft

  2. #22

    Default

    Man your cruising along! looks good so far!
    Gil
    powerpro 256
    lincoln 185

Similar Threads

  1. new project. Motor base
    By dyethor in forum Heavy Equipment and Commercial Projects
    Replies: 11
    Last Post: 06-29-2013, 09:33 PM
  2. Replies: 29
    Last Post: 09-01-2012, 05:23 PM
  3. Project #1 posixPilot, Cat: Custom Welded Shop, Mobile Tool Base
    By posixPilot in forum Other Custom Fabrications
    Replies: 0
    Last Post: 04-02-2012, 02:49 PM
  4. Replies: 7
    Last Post: 03-03-2012, 07:49 PM
  5. 1968 Chevy C-10, project #5, d.fisher
    By d.fisher in forum Truck, Car and Bike builds
    Replies: 18
    Last Post: 02-29-2012, 07:13 PM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •