    Default Holding fixture to join filler rods

    Anybody got any good ideas for a holding fixture to join short pieces of filler rod?
    Everlast PowerTig 200DX
    Snapon FM140 Mig
    Purox Oxy/Acet Torch
    Coleman 80 gal. Compressor
    7x10 Mini Lathe
    Craftsman 12" Bandsaw
    Lots of litler stuff

  2. #2

    Default

    A pair of "helping hands" might work. Those weighted stands with two jointed clip arms. They've worked everytime I've ever needed to join electrical wire of just about any size 10ga or under so I dont see using them to hold filler wire being too hard. You could also try laying them in an in 90ยค trough made by two ceramic blocks.(Used that type of setup for small joints before.)

  3. #3

    Default

    Yea, Im kinda thinking of laying it down inside a 90 degree angle with a hole or gap in the center.
    Everlast PowerTig 200DX
    Snapon FM140 Mig
    Purox Oxy/Acet Torch
    Coleman 80 gal. Compressor
    7x10 Mini Lathe
    Craftsman 12" Bandsaw
    Lots of litler stuff

  4. #4

    Default

    No need for a fixture just touch them together and tack.
    This past weekend I was fabricating/welding up a new collector back, side exit exhaust for one of my son's 07 cbr600rr. Click image for larger version. 

Name:	425113_10151340519980531_512170530_23077115_351853892_n.jpg 
Views:	385 
Size:	128.9 KB 
ID:	5551 We also installed a cbr1000 subframe. The whole bike will get painted soon.
    I had some short 1/16" tungsten on the bench that needed grinding. When I picked them up I grabbed a short piece of 1/16" 308L filler rod by mistake and sharpened it with the rest. Later on it wound up in my torch and I got a helluva surprise when I lit it up at 40 amps. It melted back to my gas lens instantly with a bright yellow light. No damage done, lesson learned.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  5. #5

    Default

    Everytime I try that they keep rolling on me, especially when the gas preflows.
    Everlast PowerTig 200DX
    Snapon FM140 Mig
    Purox Oxy/Acet Torch
    Coleman 80 gal. Compressor
    7x10 Mini Lathe
    Craftsman 12" Bandsaw
    Lots of litler stuff

  6. #6

    Default

    Quote Originally Posted by Buzz View Post
    Everytime I try that they keep rolling on me, especially when the gas preflows.
    You could stand one piece in a block of wood or something and hold the other straight down on it while you tack.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  7. #7

    Default

    Good idea! I'll try it.
    Everlast PowerTig 200DX
    Snapon FM140 Mig
    Purox Oxy/Acet Torch
    Coleman 80 gal. Compressor
    7x10 Mini Lathe
    Craftsman 12" Bandsaw
    Lots of litler stuff

  8. #8

    Default

    Wood doesnt contuct elec
    Everlast PowerTig 200DX
    Snapon FM140 Mig
    Purox Oxy/Acet Torch
    Coleman 80 gal. Compressor
    7x10 Mini Lathe
    Craftsman 12" Bandsaw
    Lots of litler stuff

  9. #9

    Default

    Quote Originally Posted by Buzz View Post
    Wood doesnt contuct elec
    It doesn't need to with a hole drilled all the way through.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  10. #10

    Default

    zoama I'm still laughing that is classic Gas stainless arc welding lol. I could picture the look on someones face when the torch flared up.
    Everlast PowerTig 250EX
    Everlast PowerCool 300
    Everlast PowerPlasma 70
    Lincoln Powermig 215
    Magnum SG Spool Gun
    Don't jump on my Gomba

  11. #11

    Default

    Quote Originally Posted by Cippee View Post
    zoama I'm still laughing that is classic Gas stainless arc welding lol. I could picture the look on someones face when the torch flared up.
    It was definitely a WTF moment.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  12. #12

    Default

    LOL at the stainless tungsten electrodes. That could make for a nice little prank for someone.

    Anyways, back on subject. I've welded together a bunch of pieces of 1/16 308l filler by just taking on a piece of aluminum. I used something like 10 or 15 amps and held the 2 pieces with my left hand. I don't have to worry about being fried by a high frequency start because I only have lift start. It works just fine once you find the right amperage.
    Everlast lx225
    Hobart Handler 210 with spool gun
    Hobart Stickmate LX
    Thermal Arc 400GMS
    40 amp Northern Tools plasma torch
    130 chicago electric tig welder
    90 amp chicago electric flux mig
    10"-22" Grizzly lathe
    15"-5.5" Grizzly vertical end mill

    In need of nice TIG machine. drooling over PowerTig 250ex

  13. #13
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    813

    Default

    Just weld one filler rod "stub" onto any workpiece, which you need to weld with that type (alloy and diameter) of filler rod. Let the puddle freeze with the filler rod stuck in the frozen puddle. It will support the filler rod rigidly and make a good ground connection.

    Grab your next filler rod stub (or even a fresh, full length, 36" long filler rod), but its end up to the end of the stub being held in the air by your workpiece, and fuse the filler rods together using your tig torch and low amps (throttling back with the footpedal is helpful, if your pedal range works at low amperages.) After your new elongated filler rod has solidified (and perhaps cooled down a bit, if you were thinking about grabbing it right where it was liquified), you are ready to continue welding on your workpiece.
    Last edited by jakeru; 03-01-2012 at 04:24 AM.
    '13 Everlast 255EXT
    '07 Everlast Super200P

  14. #14

    Default

    Another good Idea!
    Quote Originally Posted by jakeru View Post
    Just weld one filler rod "stub" onto any workpiece, which you need to weld with that type (alloy and diameter) of filler rod. Let the puddle freeze with the filler rod stuck in the frozen puddle. It will support the filler rod rigidly and make a good ground connection.

    Grab your next filler rod stub (or even a fresh, full length, 36" long filler rod), but its end up to the end of the stub being held in the air by your workpiece, and fuse the filler rods together using your tig torch and low amps (throttling back with the footpedal is helpful, if your pedal range works at low amperages.) After your new elongated filler rod has solidified (and perhaps cooled down a bit, if you were thinking about grabbing it right where it was liquified), you are ready to continue welding on your workpiece.
    Everlast PowerTig 200DX
    Snapon FM140 Mig
    Purox Oxy/Acet Torch
    Coleman 80 gal. Compressor
    7x10 Mini Lathe
    Craftsman 12" Bandsaw
    Lots of litler stuff

  15. #15

    Default

    Quote Originally Posted by Buzz View Post
    Everytime I try that they keep rolling on me, especially when the gas preflows.
    Get a quality regulator to eliminate the puff of gas, then you can join them right on the bench.
    Todd

  16. #16

    Default

    Quote Originally Posted by jakeru View Post
    Just weld one filler rod "stub" onto any workpiece, which you need to weld with that type (alloy and diameter) of filler rod. Let the puddle freeze with the filler rod stuck in the frozen puddle. It will support the filler rod rigidly and make a good ground connection.

    Grab your next filler rod stub (or even a fresh, full length, 36" long filler rod), but its end up to the end of the stub being held in the air by your workpiece, and fuse the filler rods together using your tig torch and low amps (throttling back with the footpedal is helpful, if your pedal range works at low amperages.) After your new elongated filler rod has solidified (and perhaps cooled down a bit, if you were thinking about grabbing it right where it was liquified), you are ready to continue welding on your workpiece.
    Definately have to try this! good pointer!
    Gil
    powerpro 256
    lincoln 185

  17. #17

    Default

    I took a piece of brass, (or it could be aluminum-bronze), and milled a channel with an 1/8" ball end mill. I made the channel about .150" deep and in the center of the piece I took a larger ball end mill and made a deeper area where I join the rods.

    The deeper basin does a good job collecting and holding argon but I made it a little too big and deep. I made it about .200" deep and about 3/8" wide. It only needs to be a little wider and deeper than the channel.

    Other than needing something to either hold down or prop up the other end of the long piece it works pretty good.

    Click image for larger version. 

Name:	P3020001.jpg 
Views:	433 
Size:	146.5 KB 
ID:	5648Click image for larger version. 

Name:	P3020005.jpg 
Views:	399 
Size:	151.4 KB 
ID:	5649
    Last edited by Jetfire3; 03-03-2012 at 10:53 AM.
    PowerTIG 250EX
    Power Cool 300
    Hobart 210MVP

Similar Threads

  1. Split 3/32" filler rod into two ~0.046" rods?
    By Welderooni in forum TIG Welding (GTAW/GTAW-P)
    Replies: 20
    Last Post: 08-02-2013, 03:24 PM
  2. Replies: 4
    Last Post: 11-09-2012, 01:15 AM
  3. Rods to have on hand... which ones?
    By Trip59 in forum Stick Welding (SMAW)
    Replies: 29
    Last Post: 10-13-2012, 02:44 PM
  4. Filler rod holding device!
    By 7FC_Driver in forum Other Custom Fabrications
    Replies: 2
    Last Post: 04-06-2012, 12:58 PM
  5. I'm not going to win as I won't join Facebook
    By Steve in forum Everlast Announcements, Contests and Promotions
    Replies: 6
    Last Post: 08-31-2011, 11:24 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •