I've been practicing running some 5p 6010s vertical up hill and can't figure out why the rod starts finger nailing about half way through the rod. Its so bad at times that I have to have the rod darn near vertical trying to compensate. I haven't had any issues with using the rod in any other position. I've tried moving around the ground clamp thinking that it was arc blow, but it didn't help.
I'm using 1/8'' lincoln 5p 6010s at 85 amps and about 30% dig. I'm using 1/4 inch steel.