Hello,
This is a trade show display I made for our sales guys. It consists of a heavy base that can be picked up with a forklift from any side via built in forklift fork tubes. An arm and tray that holds a demo gas tank. A machine we call a rhino drain. This project took 4 weeks to complete.
The base is made of a frame that uses 4"x6"x 1/4 tubing for the sides. 4"x 8" x 1/4" tubing for the forklift tubes. A 4'x8' x1/4 sheet steel for the deck surface. A 5"x5" x1/4" for the machine mount post. Some 1/2 plate cut to various bracing shapes.
Here is the frame for the base. this 2/3 welded. I used a Mig machine for all the welding.
This is the first pass done with a tig maching. This part a corner on the tank holding arm.
This is the top part of the tank holding arm.
Another shot of the holding arm.
This is the arm mounted onto the base. It is hinged on one side of the base plate and has the two bolts to bolt it into place. I made it hinged to make it mo0re compact for shipping.



 
					
					 
							
						 Project #5 Dyethor trade show display
 Project #5 Dyethor trade show display
		 
				
				
				