Hello. Today my project is a gasoline processing table made out of aluminum.
All the square tubing is 1"x1"x 1/8" 6061.
The channel is a 3" x 1.5" 6061.
The angle is 1.25" x 1.25" 6061.
The sheet is 1/8 thick 6061.
This table is used to first hold gas then fillter is out and send it to a big holding tank, which is usually 1000 gallons.
This first picture is cutting the metal on the band saw. I like to use this sliding square to set the proper dimension, it gives perfect repeatable results.
This is all the metal cut and awaiting to be welded into the table frame.
Here is the results of the first critical weld with my new power tig 225lx.
The second weld ready to be welded.
Two legs in the 90 degree clamps waiting to be welded.
![]()




Reply With Quote