  1. #1

    Default Project 2 from welderdude: custom tv wall mount.

    My parents bought a 32 inch LCD tv for their bedroom. They wanted to be able to watch tv while walking on the treadmill or watch it in bed. I fabbed up a wall mound that would mount to an outside corner and swing out in both directions.

    I used a piece of 2 inch by 1/8'' thick angle iron for the bracket that was going to be screw to the wall. The piece of tubing is a piece of scrap I had laying. Its about 18 inches long. the tubes that having the bolts going through them is 1 inch OD tubing with a 3/4 inch ID. I made 4 custom bushings out of steel that had a 3/8 ID and would fit into the tube snuggly. Its all MIG welded together. The bracket is held to the wall with 4 3'' long drywall screws. I was going to use lags, but my dad and I decided that the drywall screws were strong enough and he didn't want bigger holes in his wall.

    The bracket that is attached to the tv is 2 parts. There are 2 pieces of 3/16 by 1'' flat stock with the 4 mounting holes drilled and 4 - 1/4x28 holes that the second piece mounts to. the rest of it also uses the same size flat stock.

    pic 1 shows the tv in the position that is used for walking on the treadmill.

    pic 2 shows it close to where my mom puts it when she watched tv in bed.

    the rest are pretty self explanatory i think.
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	CIMG2886.jpg 
Views:	619 
Size:	32.8 KB 
ID:	5339   Click image for larger version. 

Name:	CIMG2887.jpg 
Views:	520 
Size:	29.8 KB 
ID:	5340   Click image for larger version. 

Name:	CIMG2891.jpg 
Views:	472 
Size:	31.9 KB 
ID:	5341   Click image for larger version. 

Name:	CIMG2892.jpg 
Views:	495 
Size:	29.9 KB 
ID:	5342   Click image for larger version. 

Name:	CIMG2893.jpg 
Views:	463 
Size:	28.7 KB 
ID:	5343  

    Everlast lx225
    Hobart Handler 210 with spool gun
    Hobart Stickmate LX
    Thermal Arc 400GMS
    40 amp Northern Tools plasma torch
    130 chicago electric tig welder
    90 amp chicago electric flux mig
    10"-22" Grizzly lathe
    15"-5.5" Grizzly vertical end mill

    In need of nice TIG machine. drooling over PowerTig 250ex

Similar Threads

  1. Custom Archery Camera Mount
    By cbmkr in forum Other Custom Fabrications
    Replies: 7
    Last Post: 08-01-2012, 03:50 PM
  2. John deere Gator TX Custom Brush Guard & Winch Mount
    By cbmkr in forum Off Road Fabrication
    Replies: 0
    Last Post: 07-15-2012, 02:35 PM
  3. Wall art , first real tig project.
    By Ram48 in forum Metal Art
    Replies: 15
    Last Post: 05-13-2012, 02:41 PM
  4. Project #1 from welderdude: parting tool holder
    By welderdude in forum Other Custom Fabrications
    Replies: 0
    Last Post: 01-27-2012, 02:42 AM
  5. Project 1 from Welderdude, a walkway addition.
    By welderdude in forum Hobyist Projects
    Replies: 2
    Last Post: 08-01-2011, 04:10 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •