Quote Originally Posted by dyethor View Post
I'm not use to a flow meter with liters per min that will take a little time to get use to tuning for different things.
geezer posted up a nice rule of thumb on that not too long ago, flow in lpm should be equal to the cup size, 1 or 2 less for a gas lens, +1 for higher amps (200 or more IIRC)