    Say, I have a Powermaster 256 and I mainly need it as a plasma cutter but I have had a lot of trouble with the cutters. The one that originally came with the welder caught on fire on the handle near the cutting electrode. Because the unit was a few months out of warranty, I had to buy another cable/cutter assembly. This one has the number SG-55 stamped on the plastic near the cutter electrode. It cuts fine for a couple of minutes and then it loses efficiency very quickly. The electrode erodes very quickly.

    When I look at the plasma cutter expendables, I don't see a cutter that looks anything like the one I have. Can I get expendables for this??? It's only about a year old. Is there another cutter/cable assembly that works better than this??

    I had a heck of a time getting the right cutter/cable when I ordered the one I have now. At first, even after sending a picture of the connector plug, I was sent the wrong one which I had to return. Mine has a separate 7-pin connector rather than the connector which is integrated into the main cable plug. I sure hope you can help me -- I've pretty much had nothing but trouble with this unit from the start.

    The original cutter which caught on fire but which worked pretty good for a while had a little metal guide on it to maintain the proper distance between the cutter and the work-piece. Are these available for this SG-55 cutter I have?

    Thanks!

    Eric Treider

  2. #2

    Default

    Quote Originally Posted by The_Postman View Post
    Say, I have a Powermaster 256 and I mainly need it as a plasma cutter but I have had a lot of trouble with the cutters. The one that originally came with the welder caught on fire on the handle near the cutting electrode. Because the unit was a few months out of warranty, I had to buy another cable/cutter assembly. This one has the number SG-55 stamped on the plastic near the cutter electrode. It cuts fine for a couple of minutes and then it loses efficiency very quickly. The electrode erodes very quickly.

    When I look at the plasma cutter expendables, I don't see a cutter that looks anything like the one I have. Can I get expendables for this??? It's only about a year old. Is there another cutter/cable assembly that works better than this??

    I had a heck of a time getting the right cutter/cable when I ordered the one I have now. At first, even after sending a picture of the connector plug, I was sent the wrong one which I had to return. Mine has a separate 7-pin connector rather than the connector which is integrated into the main cable plug. I sure hope you can help me -- I've pretty much had nothing but trouble with this unit from the start.

    The original cutter which caught on fire but which worked pretty good for a while had a little metal guide on it to maintain the proper distance between the cutter and the work-piece. Are these available for this SG-55 cutter I have?

    Thanks!

    Eric Treider
    Eric

    consumables you need you can find here http://www.everlastgenerators.com/Pl...cts.php?id=128

    call me at the office and i will give you batter price on consumables
    Oleg Gladshteyn
    Phone: 650 588 8082 / 877 755 WELD
    Cell: 415 613 6664 ONLY IF YOU REALLY NEED IT
    Email: oleg@everlastwelders.com
    Website www.everlastgenerators.com

    www.linkedin.com/pub/oleg-gladshteyn/48/b08/875

  3. #3

    Default

    Check out this site for pictures regarding that model : http://www.river-weld.com/Supply-sg55_c1717
    Some of those lies people tell about me, are true

  4. #4

    Default

    If you have moisture in your air compressor, the wrong air pressure or wrong stand off, the consumables "will" go rather quickly. Also you can damage the torch. You mention your cutter died, but I think you meant your plasma torch burnt up.

    Run your air between 65-70, add a water separator or dryer (that will help a lot of how long they last). Also, check with sales and get the stand off ring and use that until you get the right feel for distance. Make sure you do not see any moisture in the water trap, if you do add a desiccant type filter right behind the cutter.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  5. #5
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    Quote Originally Posted by everlastsupport View Post
    add a desiccant type filter right behind the cutter.
    Wouldn't that be before the machine?
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

  6. #6

    Default

    Quote Originally Posted by redbeard View Post
    Wouldn't that be before the machine?
    Yes. Right at the back of the machine. Though I have a bigger unit at the compressor, a small dryer there work great for me.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  7. #7

    Default

    Good advice. I think that an air dryer should be mandatory with any plasma cutter because moisture will wreak havoc with your electrodes. I would hate to fight the type of humidity they have down south when running a compressor.
    My review on Youtube of the Everlast Powermaster 205
    http://www.youtube.com/watch?v=Sih-V...7&feature=plcp
    Just a noob having fun with metal.

Similar Threads

  1. 256 plasma problems
    By Charkilah in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 2
    Last Post: 11-08-2012, 09:03 PM
  2. Power Plasma 50 plasma cutter....
    By CGCINC in forum Customer Testimonials
    Replies: 4
    Last Post: 07-20-2012, 12:58 PM
  3. Plasma Problems
    By Slartybartfa in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 34
    Last Post: 07-03-2012, 02:03 AM
  4. Problems with plasma cutter
    By Kodiak in forum Everlast Plasma Cutters (PAC)
    Replies: 10
    Last Post: 04-11-2012, 07:19 PM
  5. Problems with plasma cutter
    By Jef_Replogle in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 20
    Last Post: 03-15-2012, 10:03 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •