    Default Welding together the first 2 pieces

    These photos are better explained in the stick welding section.

    Arc force max:



    Arc force min:

    "It's not magic it's experimental, kind of like washing your hands after pooping used to be." -House

    Everlast PowerTig 250EX-arrived 1-26-2012
    Everlast PowerCool W300-arrived 1-26-2012
    Everlast PowerTig 185 Micro-arrived 1-26-2012
    Everlast PowerPlasma 70-arrived 1-26-2012
    ESAB MigMaster 250-borrowed
    HyperTherm 151 AKA "The Light Sabre"
    Linde UCC-305-964 lb. of old time water cooled TIG love-SOLD-Bad MOJO
    Purox OXY/ACETYLENE

  2. #2
    Join Date
    Feb 2011
    Location
    Fridley, Minnesota
    Posts
    376

    Default Finished Prototype. Improvements to come!!

    I finally got down to business and got this finished to the point where I can use it and see where I need to go from here. Below are a few shots of what I came up with.





    I plan to modify this for more precision placement of the engine, but the tilt seen here will make for easy assembly of the gear chest without things falling out.



    Left/Right articulation will aid in cylinder assembly, and combined with the back/forth movement, will aid in cc'ing the combustion chambers, which was the original idea behind the whole project.





    So what do you think? Future improvements will be to lower the whole assembly so that the center of gravity is closer to the rotating axis of the engine stand, making the unit more stable, and safer. (I would NEVER offer this unit for sale to the public as it is now, due to safety issues). And I think that I can simplify the design to make it easier to make.

    Next up is a transmission adapter to mount the tranny in much the same way. Rebuilding a Harley tranny requires manipulating the box in several different angles just like the engine.

    Feedback anyone??
    "It's not magic it's experimental, kind of like washing your hands after pooping used to be." -House

    Everlast PowerTig 250EX-arrived 1-26-2012
    Everlast PowerCool W300-arrived 1-26-2012
    Everlast PowerTig 185 Micro-arrived 1-26-2012
    Everlast PowerPlasma 70-arrived 1-26-2012
    ESAB MigMaster 250-borrowed
    HyperTherm 151 AKA "The Light Sabre"
    Linde UCC-305-964 lb. of old time water cooled TIG love-SOLD-Bad MOJO
    Purox OXY/ACETYLENE

Similar Threads

  1. Project 1 From Hooda Tranny case repair (FOR 1st 2013)
    By hooda in forum On Road Fabrication
    Replies: 19
    Last Post: 01-22-2013, 06:23 AM
  2. Project #2-3 From Hooda-Caravan engine rehab
    By hooda in forum Personal Projects (no welder required)
    Replies: 4
    Last Post: 02-17-2012, 03:58 AM
  3. Project #1-3 Form Hooda-Snowblower modification
    By hooda in forum Personal Projects (no welder required)
    Replies: 5
    Last Post: 12-25-2011, 07:37 PM
  4. Project #6 from Hooda- Mower deck weld reinforce
    By hooda in forum Welding Repairs
    Replies: 0
    Last Post: 10-24-2011, 03:53 AM
  5. Project #5 from Hooda- Springer front fork restore
    By hooda in forum On Road Fabrication
    Replies: 5
    Last Post: 10-23-2011, 03:07 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •