Share
Results 1 to 20 of 26

Thread: DIY Telescoping Round Tube

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. Default

    Paul the pickling will remove the black oxidation and surface rust correct?
    PowerPro 205
    9" South Bend Lathe
    Enco Mill/Drill
    Evolution Rage 2

  2. #2
    Join Date
    Oct 2010
    Location
    Nova Scotia, Canada
    Posts
    143

    Default

    Yes.

    If you've got some of the real heavy black stuff similar to stuff that's badly oxidized (sugaring / popcorn on unsheilded side) that will be hard to entirely remove. But 99% will come off with a quick wire brushing or just a manual scotchbrite pad scrub while you're neutralizing the pickle juice. (Use baking soda & water).

    The only issue is with pinholes or other crevices which will cause pitting corrosion, producing rust spots.

    Wear gloves if you don't want to have yellow nails and eye protection if you like seeing!

  3. Default

    Thanks Paul and I am very familliar with the PPE for acids.
    PowerPro 205
    9" South Bend Lathe
    Enco Mill/Drill
    Evolution Rage 2

  4. #4
    Join Date
    Oct 2010
    Location
    Nova Scotia, Canada
    Posts
    143

    Default

    If only I'd follow my own advice....

    (I guess that makes me a safety hypocrite?)

  5. Default

    I hear you, I usually need a reminder every so often usually as a burning feeling on my hand or some new holes in my jeans. I also work with hydrogen peroxide and that is always fun.
    PowerPro 205
    9" South Bend Lathe
    Enco Mill/Drill
    Evolution Rage 2

Similar Threads

  1. Tube welding question
    By agent4573 in forum General Welding Questions
    Replies: 8
    Last Post: 04-06-2013, 01:01 PM
  2. Cutting Stainless round bar with a band saw.......?
    By CGCINC in forum General Welding Questions
    Replies: 30
    Last Post: 06-02-2012, 01:35 PM
  3. Project 3 by redbeard: Telescoping Legs
    By redbeard in forum Hobyist Projects
    Replies: 0
    Last Post: 10-25-2011, 06:39 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •