  1. #1

    Default Welding copper and copper alloys

    I like welding copper and it's alloys. I like this video and though I would share it. You want a test weld a 1/2" copper pipe using a 14 gauge copper wire as filler metal. It's quite tricky. Silicon bronze is easier to weld then copper though. When ever I have to weld copper or it's alloys I'm happy. However I don't like brass the zinc sucks and will make you sick.

    http://www.youtube.com/v/12Q0uejml7s?autoplay=1
    Last edited by Cippee; 02-20-2012 at 06:13 PM.
    Everlast PowerTig 250EX
    Everlast PowerCool 300
    Everlast PowerPlasma 70
    Lincoln Powermig 215
    Magnum SG Spool Gun
    Don't jump on my Gomba

  2. #2

    Default

    Is that you Cippee? Good video.. It amazes me how steady some peoples hands are.
    Everlast PowerPlasma70
    Hobart Ironman 230
    Lincoln A-D/C 225
    'Classic' Everlast Powertig 200DX 'We don't need no steenkin pre-flow..'
    jakemateer.com

  3. #3

    Default

    No it isn't me I don't have that steady of hands either. I think it's off a miller advanced tig welding techniques. I would have to prop to steady my hands.
    Everlast PowerTig 250EX
    Everlast PowerCool 300
    Everlast PowerPlasma 70
    Lincoln Powermig 215
    Magnum SG Spool Gun
    Don't jump on my Gomba

  4. #4

    Default

    It's Ron Covell. He is a pretty well known metal working instructional video guy. Has a bunch of stuff related to auto restoration and fabrication available.
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

  5. #5

    Default

    No kidding. It didn't even look like his arms were braced on anything.

  6. #6

    Default

    I actually tried the same thing. Ill post a picture if I can find the piece of pipe. What's amazing is how much amperage it takes to form a puddle. for the 1/2 inch pipe, I used somewhere around 60 to 80 amps.
    Everlast lx225
    Hobart Handler 210 with spool gun
    Hobart Stickmate LX
    Thermal Arc 400GMS
    40 amp Northern Tools plasma torch
    130 chicago electric tig welder
    90 amp chicago electric flux mig
    10"-22" Grizzly lathe
    15"-5.5" Grizzly vertical end mill

    In need of nice TIG machine. drooling over PowerTig 250ex

  7. #7

    Default

    Yeah and I love how the pipe starts to glow red..
    Everlast PowerTig 250EX
    Everlast PowerCool 300
    Everlast PowerPlasma 70
    Lincoln Powermig 215
    Magnum SG Spool Gun
    Don't jump on my Gomba

  8. #8

    Default

    Here are some pictures of my attempt at welding a piece of 1/2 inch copper pipe. Its kind of weird because the puddle is kind of gummy. it doesn't flow very well along with the fact that its so darn conductive. I need to try it with a sheet of copper because I had more trouble with the fact its round than the fact that its copper.
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	CIMG2917.jpg 
Views:	563 
Size:	28.2 KB 
ID:	5284   Click image for larger version. 

Name:	CIMG2918.jpg 
Views:	594 
Size:	31.5 KB 
ID:	5285  
    Everlast lx225
    Hobart Handler 210 with spool gun
    Hobart Stickmate LX
    Thermal Arc 400GMS
    40 amp Northern Tools plasma torch
    130 chicago electric tig welder
    90 amp chicago electric flux mig
    10"-22" Grizzly lathe
    15"-5.5" Grizzly vertical end mill

    In need of nice TIG machine. drooling over PowerTig 250ex

  9. #9

    Default

    It came out pretty good.

    Did you TIG that? What gas did you use, machine settings, etc?

  10. #10

    Default

    Next time I need to work on the plumbing in my house, maybe I'll just TIG the pipes back together instead of using that nasty solder.


  11. #11

    Default

    I did that a couple of months ago. I used my gms 400 on lift tig. I don't have a pedal for it either.
    I had a cheap not so flexible wp 9 torch with a 1/16 ceriated tungsten sharp.
    I used pure argon at 15 CFH with a #5 cup.
    I was around 60 to 80 amps. I don't remember exactly though. I just know it takes A LOT of heat to get it to work. I couldn't imagine trying to tig even 1/8'' copper yet alone anything thicker.
    Everlast lx225
    Hobart Handler 210 with spool gun
    Hobart Stickmate LX
    Thermal Arc 400GMS
    40 amp Northern Tools plasma torch
    130 chicago electric tig welder
    90 amp chicago electric flux mig
    10"-22" Grizzly lathe
    15"-5.5" Grizzly vertical end mill

    In need of nice TIG machine. drooling over PowerTig 250ex

  12. #12

    Default

    >> "I couldn't imagine trying to tig even 1/8'' copper yet alone anything thicker."

    What size was that pipe you just showed pics of?

  13. #13
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    Quote Originally Posted by jp2code View Post
    Next time I need to work on the plumbing in my house, maybe I'll just TIG the pipes back together instead of using that nasty solder.

    And just think of all that money you'll save on fittings!
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

  14. #14
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    Quote Originally Posted by jp2code View Post
    >> "I couldn't imagine trying to tig even 1/8'' copper yet alone anything thicker."

    What size was that pipe you just showed pics of?
    Should be either .028(type M) or .040(type L) wall thickness.
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

  15. #15

    Default

    Ill post some pics on this thread tomorrow when I can take pics at work. I made some distillation parts out of copper all tig welded. I like to use a bronze filler rod if the joint doesn't need to be aesthetically pleasing, otherwise I use cut up a sheet of copper into thin strips and use them as filler rod.
    Power tig 225lx
    Hand tools up the wazoo.

  16. #16

    Default

    You can use copper wire also. 14ga works good.
    Everlast PowerTig 250EX
    Everlast PowerCool 300
    Everlast PowerPlasma 70
    Lincoln Powermig 215
    Magnum SG Spool Gun
    Don't jump on my Gomba

  17. #17

    Default

    Yea I've used copper wire but there are different alloys and they hardly ever give whats mixed in. I like to know what I'm burnin so I'm not like hey that flows nice but I have no idea what it is.
    Power tig 225lx
    Hand tools up the wazoo.

  18. #18

    Default

    Its not the best looking welds. These were my first go on copper with a tig machine. Previously I had only been using silver.
    Power tig 225lx
    Hand tools up the wazoo.

  19. #19
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    Quote Originally Posted by dyethor View Post
    Its not the best looking welds. These were my first go on copper with a tig machine. Previously I had only been using silver.
    So what kind of hooch you brewing with that setup?
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

  20. #20

    Default

    Its for water. It was an old setup. My current setup is all stainless steel besides some internal copper stuff. Its out put can go up to 94-95% pure ethanol, That's about as high as you can go without a vacuum setup. I do have some rum aging with vanilla bean up on the shelf. All for cleaning purposes of course.
    Power tig 225lx
    Hand tools up the wazoo.

Similar Threads

  1. Tried my hand at copper welding today
    By Kevin Caron in forum Metal Art
    Replies: 7
    Last Post: 11-06-2014, 11:10 AM
  2. Fun with copper
    By Gwaltnak in forum Hobyist Projects
    Replies: 12
    Last Post: 11-06-2013, 04:12 AM
  3. Copper Butterflies
    By dawjr32223 in forum Metal Art
    Replies: 6
    Last Post: 01-25-2013, 06:41 PM
  4. Tig Welding Grounding Bar Copper to Steel
    By cbmkr in forum TIG Welding (GTAW/GTAW-P)
    Replies: 0
    Last Post: 12-12-2012, 05:04 PM
  5. Thin gauge copper welding
    By jakeru in forum Other Custom Fabrications
    Replies: 0
    Last Post: 03-04-2011, 09:16 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •