For everyone that has dialed in there Everlast welder to leave beautiful welds on aluminum, what are your settings? It will be interesting to compare the 30/70 to the 10/90 setups.
My 250EX is set at 40 hertz, ac balance 10%, pulser at 500pps, pulse time on 50%, background current varies with amperage needed but usually 50%, start amps 35, upslope 2.5 or 25%, Regulator at 7 L/MIN with large gas lens with short cup, red 2% thoriated ground sharp then a flat ground on the end about .050 diameter.
I weld the same parts over and over again so my setting do not change much, This is the setup where mine will weld like butter but I would like to try other setups.




Reply With Quote