  1. Default

    Quote Originally Posted by sportbike View Post
    What is the benefit of using 500pps pulse all of the time?
    The fast pulse keeps the arc from wandering on low frequency's. The lower frequency's give a softer arc and the pulse just keeps it focused without making it harsh like the higher frequency's will, also average temperature of the arc will be reduced, so heat saturation will be less with pulse. The round aluminum parts I weld start with 130 amps and by the time I get all the way around them I am at 50 amps to keep the same bead width where they meet. That's without pulse and with pulse I start at 130 and end at 90 amps to have the same bead width.

  2. #2

    Default

    Quote Originally Posted by srp View Post
    The round aluminum parts I weld start with 130 amps and by the time I get all the way around them I am at 50 amps to keep the same bead width where they meet.
    That's because the part heats up?
    Everlast PowerPlasma70
    Hobart Ironman 230
    Lincoln A-D/C 225
    'Classic' Everlast Powertig 200DX 'We don't need no steenkin pre-flow..'
    jakemateer.com

Similar Threads

  1. New PowerMTS 251Si videos posted by Kevin and ChuckE
    By performance in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 6
    Last Post: 08-06-2015, 02:49 AM
  2. Replies: 1
    Last Post: 06-19-2012, 09:46 PM
  3. Editing thread title, my thread
    By worntorn in forum Forum related Questions
    Replies: 10
    Last Post: 06-20-2011, 07:03 PM
  4. About the Introduce yourself thread.
    By everlastsupport in forum Introduce Yourself
    Replies: 0
    Last Post: 07-31-2009, 11:22 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •