Quote Originally Posted by srp View Post
I weld billet end caps to .065 aluminum round tubing and then 1/4 plate mounting tabs to the .065 round tubing. I have found a softer weld similar to like a sine wave machine looks best, but with the inverter I can get that look without the cup glowing and burning off the end of the tungsten.
I tried those setting and they do produce a nice job. I also switched up on the wave form while trying that and discovered the Tri wave really looked sweet set like that... The Dynasty just give a few more tools in the belt to borrow one of Jody's lines from tips and tricks.. Every extra tool helps a guy find something that works best...