    Just a quick question. I looked around and haven't been able to find one mention of it. How many of you use CO2 for shielding gas on steel? Or better yet what type of shielding gas do you use for different types of metals?

    I use CO2 for steel, and Argon/helium for aluminum and stainless steel.
    Power tig 225lx
    Hand tools up the wazoo.

  2. #2

    Default

    I use 75/25 on my bigger mig. I have a little baby mig and I use co2 to bump up its power a tad. When I weld alm. it's 100% argon and stainless is a tri mix.
    Everlast PowerTig 250EX
    Everlast PowerCool 300
    Everlast PowerPlasma 70
    Lincoln Powermig 215
    Magnum SG Spool Gun
    Don't jump on my Gomba

  3. #3

    Default

    If you are using spray transfer instead of short circuit welding, use 98% argon 2% oxygen or 90% argon 10% co2. Trimix is 90% helium, 7.5% argon and 2.5% co2. I almost always use regular 75 25 for short circuit transfer on steel.
    Everlast lx225
    Hobart Handler 210 with spool gun
    Hobart Stickmate LX
    Thermal Arc 400GMS
    40 amp Northern Tools plasma torch
    130 chicago electric tig welder
    90 amp chicago electric flux mig
    10"-22" Grizzly lathe
    15"-5.5" Grizzly vertical end mill

    In need of nice TIG machine. drooling over PowerTig 250ex

  4. #4

    Default

    I use my Arc machine whenever I want to weld mild steel. The DC TIG is only for stainless. I used an Argon/CO2 mix at one point, but I think it welds nicer with 100% argon.

  5. #5

    Default

    Quote Originally Posted by jp2code View Post
    I use my Arc machine whenever I want to weld mild steel. The DC TIG is only for stainless. I used an Argon/CO2 mix at one point, but I think it welds nicer with 100% argon.
    Are you mig welding with pure argon?
    Everlast lx225
    Hobart Handler 210 with spool gun
    Hobart Stickmate LX
    Thermal Arc 400GMS
    40 amp Northern Tools plasma torch
    130 chicago electric tig welder
    90 amp chicago electric flux mig
    10"-22" Grizzly lathe
    15"-5.5" Grizzly vertical end mill

    In need of nice TIG machine. drooling over PowerTig 250ex

  6. #6

    Default

    Quote Originally Posted by welderdude View Post
    Are you mig welding with pure argon?
    MIG? Oh yeah! I forgot all about my MIG machine. It is tucked away in the corner of my garage and hasn't seen much use in a while. Maybe that was what I had that argon/co2 mixture for.

  7. #7

    Default

    I hoe you didn't use co2 with tig a no no. It eats the tungsten.
    Everlast PowerTig 250EX
    Everlast PowerCool 300
    Everlast PowerPlasma 70
    Lincoln Powermig 215
    Magnum SG Spool Gun
    Don't jump on my Gomba

  8. #8

    Default

    Quote Originally Posted by Cippee View Post
    I hoe you didn't use co2 with tig a no no. It eats the tungsten.
    Oh, I probably did.

    Sometimes, I feel like if I don't learn by my mistakes, I don't learn at all.

    Thick forehead, or something like that.

  9. #9

    Default

    Oh, I see what you mean. I was getting a little scared at first because I know from playing around that MIGing steel with pure argon just doesn't work.
    Everlast lx225
    Hobart Handler 210 with spool gun
    Hobart Stickmate LX
    Thermal Arc 400GMS
    40 amp Northern Tools plasma torch
    130 chicago electric tig welder
    90 amp chicago electric flux mig
    10"-22" Grizzly lathe
    15"-5.5" Grizzly vertical end mill

    In need of nice TIG machine. drooling over PowerTig 250ex

  10. #10

    Default

    Quote Originally Posted by dyethor View Post
    J How many of you use CO2 for shielding gas on steel? I use CO2 for steel, and Argon/helium for aluminum and stainless steel.
    CO2 is not the preferable shielding gas for mig welding. It works, but its more for times when your in a jam. Hobart sells a small CO2 tank with their passport 180, but they emphasize CO2 in a jam.
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  11. #11

    Default

    I've been using it without any observable problems. I weld from 20 gauge to 1" steel. What makes it un-preferable?
    Power tig 225lx
    Hand tools up the wazoo.

  12. #12

    Default

    Does anyone have any experince with using pure argon on sheet metal? I have heard it was better/worked on sheet metal.
    Everlast PowerTIG 200 DX
    Everlast Power IMIG 140

  13. #13

    Default

    Quote Originally Posted by SeanMurphy265 View Post
    CO2 is not the preferable shielding gas for mig welding. It works, but its more for times when your in a jam. Hobart sells a small CO2 tank with their passport 180, but they emphasize CO2 in a jam.
    Have to disagree with you on that,,,if you check out offshore manufacturers advertisements on mig welders they are refered to as CO2 welders,,,75/25 gas mixes are a western norm...not so in other parts of the world...CO2 is used extensivly there...It gives a hotter burn with more penetration,,,but it also has more splatter or BB's,,,75/25 and other mix's make it nicer...

    Here is a website that explains it :http://www.alibaba.com/showroom/co2-mig-welder.html
    Last edited by geezer; 04-30-2012 at 01:01 PM.
    Some of those lies people tell about me, are true

  14. #14

    Default

    Quote Originally Posted by geezer View Post
    Have to disagree with you on that,,,if you check out offshore manufacturers advertisements on mig welders they are refered to as CO2 welders,,,75/25 gas mixes are a western norm...not so in other parts of the world...CO2 is used extensivly there...It gives a hotter burn with more penetration,,,but it also has more splatter or BB's,,,75/25 and other mix's make it nicer...

    Here is a website that explains it :http://www.alibaba.com/showroom/co2-mig-welder.html
    You're right. We use small CO2 for mobile welding or flux core if windy. Since we have a smaller tank of CO2. It welds a little like flux core.

    Iron works shops (one I know) uses flux core and gas at the same time. No spatter, hot welds too.

    It just is not as pretty all the time.

    @Jules:

    On the argon question. That would be for TIG welding, not MIG.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  15. #15

    Default

    Mike, not trying to argue but I had read it about MIG and thin sheet metal.

    I will give it try later as I have both tanks, I will post an update later.
    Everlast PowerTIG 200 DX
    Everlast Power IMIG 140

  16. #16

    Default

    Quote Originally Posted by Jules The Great View Post
    Mike, not trying to argue but I had read it about MIG and thin sheet metal.

    I will give it try later as I have both tanks, I will post an update later.
    Read the whole thread. Co2 will burn hot. You can MIG with it. But I would not use it on sheet metal. Just posting you can MIG with straight Co2.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  17. #17

    Default

    Quote Originally Posted by everlastsupport View Post
    Read the whole thread. Co2 will burn hot. You can MIG with it. But I would not use it on sheet metal. Just posting you can MIG with straight Co2.
    I meant I would try with argon but this sums it up well, as I have argon and argon mix I will just use them as they were meant to be used.

    http://www.mig-welding.co.uk/welding-gas.htm
    Everlast PowerTIG 200 DX
    Everlast Power IMIG 140

Similar Threads

  1. Tungsten type and settings help please
    By agent4573 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 3
    Last Post: 07-25-2015, 03:45 AM
  2. PP 50 shielding cup.
    By powercat in forum Everlast Plasma Cutters (PAC)
    Replies: 3
    Last Post: 09-06-2011, 02:57 PM
  3. Shielding Gas Usage Question
    By SeanMurphy265 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 10
    Last Post: 05-04-2011, 04:56 AM
  4. Shielding Gas Selection
    By performance in forum Welding articles from Professionals (knowledge database)
    Replies: 6
    Last Post: 03-22-2011, 11:08 AM
  5. Shielding gas Barb on 225LX?
    By Zoomie in forum TIG Welding (GTAW/GTAW-P)
    Replies: 24
    Last Post: 01-25-2011, 04:33 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •