					Dcen on alum is used UHP helium and a oxide free weld zone we use nitric acid with some hydroflouric acid mixed in to clean the alum prior to welding normally used on the thicker stuff but i have done down to 13 gauge on dcen  using 4043
Price out UHP helium its not cheap
				
			 
			
		 
			
			
			
				