    Default tig argon flow rate ?( l/min and/or scfh)

    all the rating i see are 15-20 cfh..

    my harris regulator came with my lincoln 180c, it has
    L/MIN and SCFH and im using it on my argon tank too.

    so what should i be at in either L/MIN or SCFH?

  2. #2

    Default

    i usually tig weld between 4-7 LPM.
    -------------------------------------------
    Spike Customs, Inc.
    Fresno, CA 93727
    ph- 559-549-RIDE(7433)
    -------------------------------------------
    -Follow me on twitter!-

  3. #3

    Default

    The first time I set the flow on the gauge-type regulator that came with my mig, I didn't realize the outer scale was in L/Min and not CFH. I was running 20 L/min for the first few days until I actually looked closely at it.
    Everlast lx225
    Hobart Handler 210 with spool gun
    Hobart Stickmate LX
    Thermal Arc 400GMS
    40 amp Northern Tools plasma torch
    130 chicago electric tig welder
    90 amp chicago electric flux mig
    10"-22" Grizzly lathe
    15"-5.5" Grizzly vertical end mill

    In need of nice TIG machine. drooling over PowerTig 250ex

Similar Threads

  1. New 250ex: gas flow continues to flow
    By Mcutler in forum TIG Welding (GTAW/GTAW-P)
    Replies: 5
    Last Post: 04-17-2018, 02:17 AM
  2. problem with argon flow for new (old) powertig 185 micro (2011)
    By jonnycowboy in forum TIG Welding (GTAW/GTAW-P)
    Replies: 4
    Last Post: 03-31-2014, 02:00 PM
  3. going rate for argon and lease rates
    By dgarnier in forum General Welder Questions
    Replies: 79
    Last Post: 12-29-2013, 05:57 PM
  4. Argon Flow Rate Conversion on Tig Calculator
    By Buggy Chief in forum TIG Welding (GTAW/GTAW-P)
    Replies: 14
    Last Post: 01-03-2012, 08:13 PM
  5. Argon gauge questions/ball type flow meter
    By Longlasting in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 13
    Last Post: 07-07-2010, 07:00 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •