    We've had a few questions on TIG starting gas settings and how to translate the flow from "cubic feet per hour" and "liters per minute". Hope this helps.
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	new25.jpg 
Views:	2623 
Size:	37.9 KB 
ID:	124  
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  2. #2

    Default

    Good info, thanks.
    Wayne

  3. #3

    Default

    Hi,

    I'm not sure what the numbers is on the guage you provided for me with my 250. I know the 304 I work on likes that little ball to be just above the 15. She starts to get ugly if you let it drop any further. Thanks for the info. I will print it out and keep it with my instruction manuel.
    Frank

    I have a 250 EX welder and several other machines and equipment to allow for small scale manufacturing and prototyping of inventions

    I am located in Oregon about 20 minutes west of Portland

  4. #4

    Default

    is there any harm in having the gas too high?
    sold my miller mig
    got a PT250EX
    saving up for a plasma cutter

  5. #5

    Default

    Quote Originally Posted by dgarnier View Post
    is there any harm in having the gas too high?
    Depending on the gas and metal, yes (porosity, just like atmospheric contamination) and no as the argon (inert) you an get away with more.

    Always stay within the recommended ranges. If you have some air movement or need a longer stick-out you can add some more gas, but enough to get the job done.

    Biggest problem you will have is your wallet though. It's gauge will be going down too
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

Similar Threads

  1. Erractic arc at low AC setting
    By Sage Hill in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 9
    Last Post: 02-14-2016, 10:59 PM
  2. AC / DC Setting is backwards?
    By JonS in forum TIG Welding (GTAW/GTAW-P)
    Replies: 3
    Last Post: 05-02-2012, 02:25 AM
  3. Pulse Setting in AC
    By Buggy Chief in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 03-30-2012, 11:25 AM
  4. ARGON and ARGON/CO2 TANK SIZES
    By everlastsupport in forum Technical Bulletins and Tips
    Replies: 47
    Last Post: 10-13-2011, 05:19 AM
  5. 250EX Amp Setting Changes??
    By CMB in forum TIG Welding (GTAW/GTAW-P)
    Replies: 8
    Last Post: 08-11-2011, 03:13 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •