    This is an odd thread to start, however. The other day I forgot to turn on the argon and when I tried to start an arc the hf just buzzed and I realized I didn't have gas. It got me think most people don't think all the time about how the gas helps the arc to form and be stable. Hence why helium is about a 1/3 hotter than argon. If you have an old tungsten try welding with pure co2 for a laugh. co2 does not like to let the arc travel through it. I believe one reason is because it is not an inert gas and has more interaction with the arc. Also you know if you don't preflow the argon the blast of pressure can mess with the arc. Well at least it you have a crappy regulator like me. You guys know alot more than me so I'm interested in hearing your ideas about this.
    Everlast PowerTig 250EX
    Everlast PowerCool 300
    Everlast PowerPlasma 70
    Lincoln Powermig 215
    Magnum SG Spool Gun
    Don't jump on my Gomba

  2. #2
    Join Date
    Jan 2010
    Location
    Chugiak , Alaska
    Posts
    259

    Default

    Well, not sure if you realize what can you opened up.
    I could, (and maybe should) write a book.

    But the very short answer is in Tig welding the gas is the arc….

    The argon is ionized and becomes the conductor, what we perceive as a flame like arc is actually an envelope of ionized argon conducting current.
    Argon is used because it’s easy to ionize because of the number of electrons in the outer shell of the atom, it’s inert and won’t react with the molten metal and it's cheap and easy to produce.
    Last edited by Ray; 02-13-2012 at 06:08 PM.
    ____
    Ray

    Everlast Sales and Support Team.
    support@everlastalaska.com
    www.everlastalaska.com

    877-755-9353 X207

  3. #3

    Default

    I was hoping to stir up something. I learn something everyday on this forum. I know in mig welding people don't like to use pure co2 as much because it is a harsher arc because like you said it doesn't ionize like argon does.
    Everlast PowerTig 250EX
    Everlast PowerCool 300
    Everlast PowerPlasma 70
    Lincoln Powermig 215
    Magnum SG Spool Gun
    Don't jump on my Gomba

  4. #4

    Default

    Well I guess this thread doesn't peak as much interest as I hoped it would. Oh well.
    Everlast PowerTig 250EX
    Everlast PowerCool 300
    Everlast PowerPlasma 70
    Lincoln Powermig 215
    Magnum SG Spool Gun
    Don't jump on my Gomba

Similar Threads

  1. 200dx frequency effect on DC welding
    By vicrc in forum TIG Welding (GTAW/GTAW-P)
    Replies: 9
    Last Post: 11-09-2012, 04:12 PM
  2. Effect of AC Balance control on aluminum
    By performance in forum Welding articles from Professionals (knowledge database)
    Replies: 4
    Last Post: 09-07-2011, 01:56 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •